Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 210 - 229 °C | 410 - 445 °F | |
Ravago Manufacturing Americas Hylac® GP55 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 210 - 229 °C | 410 - 445 °F | |
Ravago Manufacturing Americas Hylac® GP74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 210 - 229 °C | 410 - 445 °F | |
Ravago Manufacturing Americas Hylac® GP74G20 ABS, 20% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 210 - 229 °C | 410 - 445 °F | |
Ravago Manufacturing Americas Hylac® GP74G30 ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 210 - 229 °C | 410 - 445 °F | |
Ravago Manufacturing Americas Hylac® HF143 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 210 - 229 °C | 410 - 445 °F | |
Ravago Manufacturing Americas Hylac® HF224 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 210 - 229 °C | 410 - 445 °F | |
Ravago Manufacturing Americas Hylac® HF96 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 204 - 229 °C | 400 - 445 °F | |
PTS SAN-80HF High Flow SAN Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 191 - 229 °C | 375 - 445 °F | |
ExxonMobil Santoprene® 111-55 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Nozzle Temperature | 191 - 229 °C | 375 - 445 °F | |
ExxonMobil Santoprene® 111-64 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Nozzle Temperature | 191 - 229 °C | 375 - 445 °F | |
ExxonMobil Santoprene® 221-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Nozzle Temperature | 204 - 229 °C | 400 - 445 °F | |
PTS SAN-82TR SAN Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 210 - 229 °C | 410 - 445 °F | |
Ravago Manufacturing Americas Hylac® GP48 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 221 - 229 °C | 430 - 445 °F | |
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Nozzle Temperature | 221 - 229 °C | 430 - 445 °F | |
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;.. |
|||
Nozzle Temperature | 221 - 229 °C | 430 - 445 °F | |
Teknor Apex Telcar® TL-8451 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Nozzle Temperature | 221 - 229 °C | 430 - 445 °F | |
Teknor Apex Telcar® TL-8712 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Nozzle Temperature | 221 - 229 °C | 430 - 445 °F | |
Teknor Apex Telcar® TL-8730 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Nozzle Temperature | 191 - 229 °C | 375 - 445 °F | |
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Nozzle Temperature | 191 - 229 °C | 375 - 445 °F | |
ExxonMobil Santoprene® 111-73 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Nozzle Temperature | 191 - 229 °C | 375 - 445 °F | |
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Nozzle Temperature | 191 - 229 °C | 375 - 445 °F | |
ExxonMobil Santoprene® 211-55 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Nozzle Temperature | 191 - 229 °C | 375 - 445 °F | |
ExxonMobil Santoprene® 211-64 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Nozzle Temperature | 191 - 229 °C | 375 - 445 °F | |
ExxonMobil Santoprene® 211-73 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Nozzle Temperature | 191 - 229 °C | 375 - 445 °F | |
ExxonMobil Santoprene® 211-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Nozzle Temperature | 210 - 229 °C | 410 - 445 °F | |
Ravago Manufacturing Americas Hylac® GP30G ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 191 - 229 °C | 375 - 445 °F | |
ExxonMobil Santoprene® 111-87 Thermoplastic Elastomer
(discontinued **) A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Nozzle Temperature | 191 - 229 °C | 375 - 445 °F | |
ExxonMobil Santoprene® 211-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Nozzle Temperature | 191 - 229 °C | 375 - 445 °F | |
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |