Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 177 - 193 °C | 350 - 380 °F | |
Ravago Manufacturing Americas Hylac® FR74 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® J-60/10/FR Polypropylene Homopolymer, 10% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® J-60/20 Polypropylene Homopolymer, 20% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® J-60/20/FR Polypropylene Homopolymer, 20% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® J-60/20/H Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® J-60/30/E Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® J-60/30/E8/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® J-60/30/FR Polypropylene Homopolymer, 30% Glass Fiber Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® J-60/40/E Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® M-2149 Polypropylene Homopolymer, 30% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® PP-60/CC/40 Polypropylene Homopolymer, 40% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® PP-60/TC/20 Polypropylene Homopolymer, 20% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® PP-60/VO/NH Polypropylene Homopolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® PP-61/TC/20/UV Polypropylene Copolymer, 20% Talc, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® PP-61/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® PP-68/TC/20 Polypropylene Copolymer, 20% Talc Information provided by FIBERFIL Engineered Plastics |
|||
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Fiberfil® PP-68/V2 Polypropylene Copolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |