Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 249 °C | 480 °F | |
Oxford Polymers PBT 30GF PBT, 30% Glass Fiber Reinforced Product Description: Glass Fiber (30% Reinforced), PBT injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and LubricantsSpecial Characteris.. |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | |
Ravago Manufacturing Americas Hybrid S459 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | |
Ravago Manufacturing Americas Hybrid S464 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | |
Ravago Manufacturing Americas Hybrid S466 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Nozzle Temperature | 249 - 288 °C | 480 - 550 °F | |
PTS Tristar® PC-05GFR 5% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | |
Firestone C200-001 Nylon 6 Natural color. Not heat stabilized, modified, or lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | |
Firestone C212-15C Nylon 6, Heat Stabilized Off white color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | |
Firestone CL200-001 Nylon 6 Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | |
Firestone CLM200-001 Nylon 6 Used for monofiliament extrusion. Natural color. Not heat stabilized or modified. Lubricated. Chip size is 2 x 3.5 mm.Information provided by Firestone |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | |
Firestone CR212-203-D Nylon 6, Heat Stabilized Black color. Heat stabilized, Modified, and Lubricated. Chip size is 2 x 3 mm.Information provided by Firestone |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Nozzle Temperature | 249 - 271 °C | 480 - 520 °F | |
LTL Color Compounds ColorFast® FRPBT130 PBT, 30% Glass-Filled 30% glass-filled V-0 rated PBT - UL listedAll information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 249 - 271 °C | 480 - 520 °F | |
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded 13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 249 - 277 °C | 480 - 530 °F | |
LTL Color Compounds ColorFast® NY2115 Nylon 66 Super tough nylon 6,6 with excellent chemical resistance and ductilityAll information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | Injection Molding |
Ineos ABS Triax® 1185 ABS/Nylon Alloy, Injection Molding Grade Triax® 1185 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with excellent processability, good chemical resistance, g.. |
|||
Nozzle Temperature | 249 - 260 °C | 480 - 500 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Nozzle Temperature | 249 °C | 480 °F | |
MTI ThermoStran® PP-30C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Nozzle Temperature | 249 °C | 480 °F | |
MTI ThermoStran® PP-30G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Nozzle Temperature | 249 °C | 480 °F | |
MTI ThermoStran® PP-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Nozzle Temperature | 249 °C | 480 °F | |
MTI ThermoStran® PP-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Nozzle Temperature | 249 °C | 480 °F | |
MTI ThermoStran® TPU-40C Long Carbon Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Nozzle Temperature | 249 °C | 480 °F | |
MTI ThermoStran® TPU-40G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Nozzle Temperature | 249 °C | 480 °F | |
MTI ThermoStran® TPU-50G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Nozzle Temperature | 249 °C | 480 °F | |
MTI ThermoStran® TPU-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Nozzle Temperature | 249 - 254 °C | 480 - 489 °F | |
Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
Nozzle Temperature | 249 - 254 °C | 480 - 489 °F | |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Nozzle Temperature | 249 - 254 °C | 480 - 489 °F | |
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided .. |
|||
Nozzle Temperature | 249 - 271 °C | 480 - 520 °F | |
Wellman Wellamid® GF14-60 XE-N 14% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Nozzle Temperature | 249 - 271 °C | 480 - 520 °F | |
Wellman Wellamid® GF20-60 XE-N 20% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |
|||
Nozzle Temperature | 249 - 271 °C | 480 - 520 °F | |
Wellman Wellamid® GF30-60 XE-N 30% Glass Fiber Reinforced Nylon 6, Lubricated & Heat Stabilized Typical Applications: Radio and TV components, dishwasher roller carriages, chain saw oil reservoirs, gears, housings, door & window latches, power hand tool housings, high temperature devices.Data .. |