Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3N Unfilled, Nucleated PA6 Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro.. |
|||
Nozzle Temperature | 240 - 270 °C | 464 - 518 °F | |
Nilit Nilamid B3 H ZB Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZB is a high impact NYLON 6. The product has excellent impact properties, even at minus temperatures, whilst maintaining mechanical characteristics. Application areas inclu.. |
|||
Nozzle Temperature | 240 - 310 °C | 464 - 590 °F | Average value: 279 °C Grade Count:7 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Nozzle Temperature | 240 - 295 °C | 464 - 563 °F | Average value: 269 °C Grade Count:8 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | |
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | |
LG Chemical LUMAX HR-5306F Heat Resistant PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Nozzle Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP1000H PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP1000M PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® HV1005S PBT Description: Injection Molding, PBT, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 240 - 260 °C | 464 - 500 °F | |
LG Chemical Lupox® PBT-GP-2156F 15% GFR Flame Retardant PBT General Purpose PBT, 15% Glass Fiber Reinforced, Weather Resistant, Flame Retardant, Non-Bleed. Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
LG Chemical LUPOY HR-5006A Heat Resistant PC/ABS Alloy, Unreinforced, Weather Resistant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide.. |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical XR474 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior HousingCAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | |
Samyang Triloy® 120H PC/ABS alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | |
Samyang Triloy® 130 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Nozzle Temperature | 240 °C | 464 °F | |
Zhejiang Juner 301-G0 Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Nozzle Temperature | 240 °C | 464 °F | Recommended |
Arkema Group Pebax® 4033 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 4033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Nozzle Temperature | 240 - 250 °C | 464 - 482 °F | Cast Film |
Arkema Group Pebax® MV 3000 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 3000 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on .. |
|||
Nozzle Temperature | 240 °C | 464 °F | Recommended |
Arkema Group Pebax® Rnew 40R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 40R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Nozzle Temperature | 240 - 270 °C | 464 - 518 °F | |
Ascend Performance Materials Vydyne® 909 BK Nylon 66/6, 25% Glass Reinforced, DAM Vydyne® 909 BK is a halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwrite.. |
|||
Nozzle Temperature | 240 - 270 °C | 464 - 518 °F | |
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr.. |
|||
Nozzle Temperature | 240 - 245 °C | 464 - 473 °F | |
Beijing Chemical Industry KAIFA® HN301-G10 PA6 Resin 10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 240 °C | 464 °F | |
Beijing Ranger Chem PBT 403 M-G20 Heat Resistant and Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Nozzle Temperature | 240 °C | 464 °F | |
Beijing Ranger Chem PBT-201-G30 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Nozzle Temperature | 240 °C | 464 °F | |
BLUESTAR PBT 403M-G30 30% Glass Filled PBT, injection molding grade, 30% glass fiber reinforced, flame retardant, exceptional flowability and processability, colorableInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 240 - 280 °C | 464 - 536 °F | |
Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Nozzle Temperature | 240 °C | 464 °F | |
Beijing Ranger Chem PBT-201-G20 202 Environmental Protection Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Nozzle Temperature | 240 °C | 464 °F | |
Beijing Ranger Chem PBT-201-G30 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |