Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 230 °C | 446 °F | |
Inchem Phenoxy PKFE Phenoxy PKFE - polyhydroxy ether of Bisphenol A. Originally developed by Union Carbide. Produced by InChem Corporation. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT 1068D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT 3055D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical LUCON 6080EX ABS+CF Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Wide Processing RangeApplication: Carrying Cart Pipe Coating, BLU carrying TrayCAS No. 9003-56-9, 9003-54-7 and 7782-42-6Informatio.. |
|||
Nozzle Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical LUMIPLAS LD590 Light diffusion ABS Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUPOS HR-2207 Heat Resistant SAN, 20% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUPOS HR-2407 Heat Resistant SAN, 40% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by .. |
|||
Nozzle Temperature | 230 - 260 °C | 446 - 500 °F | |
Gromax 1163LL TPE 163LL is medium modulus grade with nominal Durometer hardness of 63D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ext.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical ER461 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemica.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR401T ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay TECHNYL® C 216 V15 PA6, 15% glass filled, Eh 0 Description: TECHNYL C 216 V15 is a polyamide 6 with 15% of glass fiber.Colors: it is marketed in the black color and natural.Available in: Asia Pacific and EuropeMain Properties: Dimensional stabil.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay TECHNYL® C 218 V40 PA6, 40% glass fiber, Eh 0 Description: TECHNYL C 218 V40 is a polyamide 6 with 40% of glass fiber and with thermal stability.Colors: it is marketed in the black color and natural.Available in: Latin AmericaMain Properties: ?.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | |
Samyang Tribit® 1500 Polybutylene Terephthalate Characteristics:Medium viscosityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samy.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | |
Samyang Tribit® 1503 Polybutylene Terephthalate Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | |
Samyang Tribit® 1503S Polybutylene Terephthalate Characteristics:High impactApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samyang |
|||
Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
Arkema Group Pebax® 7033 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
Arkema Group Pebax® 7033 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
Arkema Group Pebax® 7233 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7233 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
Arkema Group Pebax® Rnew 72R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 72R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Nozzle Temperature | 230 - 255 °C | 446 - 491 °F | Injection Molding |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
Arkema Group Pebax® Rnew 70R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 70R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Nozzle Temperature | 230 - 305 °C | 446 - 581 °F | Average value: 279 °C Grade Count:10 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an.. |
|||
Nozzle Temperature | 230 °C | 446 °F | Typical Die Temp. |
DuPont Nucrel® 1214 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
(discontinued 12 wt% Methacrylic Acid.Nucrel® 1214 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des.. |