Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products CC40P100-00EG 40% Calcium Carbonate Reinforced Polypropylene, Natural, Extrusion Grade Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products G40P100-00 40% Glass Fiber Reinforced Polypropylene, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products G40P100-04UV 40% Glass Fiber Reinforced Polypropylene, UV Stabilized, White Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products GC40P100-01 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products GC40P101-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products GC43P250-00 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Consumer goodsFunctional supportsHead lamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 441 - 460 °F | |
PolyOne OnFlex™ HFFR 360-0185 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 360-0185 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - Non-halogen flame re.. |
|||
Nozzle Temperature | 227 - 238 °C | 441 - 460 °F | |
PolyOne OnFlex™ HFFR 361-0190 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 361-0190 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - UL 94 HB compliantPu.. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products M40P100-00 40% Mica Reinforced Polypropylene, Natural Applications: Structural componentsAir ductsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products RCT140-01A 40% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC ductworkI/P componentsFuse panel assembliesUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P100-04 40% Talc Reinforced Polypropylene, White Applications: Automotive componentsConsumer productsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P100-774UVA 40% Talc Reinforced Polypropylene, UV Stabilized, JA6A Black Applications: Wire troughBracketsConsolesFan shroudsFuse panel boxDoor cup pullsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P105-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P106-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P108-01 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P109-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkBrackets/SupportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P200-01 40% Talc Reinforced Polypropylene Copolymer, Black Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 210 - 238 °C | 410 - 460 °F | |
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o.. |
|||
Nozzle Temperature | 200 - 238 °C | 392 - 460 °F | Average value: 219 °C Grade Count:6 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Nozzle Temperature | 216 - 238 °C | 420 - 460 °F | |
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Nozzle Temperature | 216 - 238 °C | 420 - 460 °F | |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Nozzle Temperature | 210 - 238 °C | 410 - 460 °F | |
ExxonMobil Santoprene® 103-40 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Nozzle Temperature | 210 - 238 °C | 410 - 460 °F | |
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Nozzle Temperature | 200 - 238 °C | 392 - 460 °F | Average value: 226 °C Grade Count:28 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Consumer goodsFunctional supportsHead lamp bracketsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 218 - 238 °C | 425 - 460 °F | Average value: 229 °C Grade Count:5 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |