Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT1003-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step and hitch padsInterior component and trimA/B pillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT2500-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT2500-630UV Thermoplastic Polyolefin, UV Stabilized, 500F Light Charcoal Applications: Air DamsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT2700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT3080-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT3080-727UV Thermoplastic Polyolefin, UV Stabilized, G01 Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT3080-757UV Thermoplastic Polyolefin, UV Stabilized, Pueblo Gold Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products FT4600-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products P104-00 Polypropylene, Natural Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products P249-01UV General Purpose Polypropylene Copolymer, UV Stabilized, Black Applications: LP bracketsSplash shieldsDoor/trunk scuffInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products UVP254-01 Polypropylene Copolymer, UV Stabilized, Black Applications: Fuel filler pocketInterior trimI/P componentsCenter consoleInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Versollan™ RU 2204X Thermoplastic Elastomer (TPE) Versollan™ RU 2204X is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performan.. |
|||
Nozzle Temperature | 191 - 216 °C | 376 - 421 °F | |
PolyOne Versollan™ RU 2205-1 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-1 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Nozzle Temperature | 191 - 216 °C | 376 - 421 °F | |
PolyOne Versollan™ RU 2205-9 Thermoplastic Elastomer (TPE) Versollan™ RU 2205-9 is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performa.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Nozzle Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G7930-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7930-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynaflex™ G7640-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynalloy™ OBC 8100-N50 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N50 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Nozzle Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynalloy™ OBC 8100-N65 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N65 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC SunPro® SP 200 P 3085 Polypropylene Copolymer SunPro® SP 200 P 3085 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM.PP... |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC SunPro® SP 200 P 5000 Polypropylene Copolymer SunPro® SP 200 P 5000 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: MS DB5.. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC SunPro® SP 200 P3081 Polypropylene Copolymer SunPro® SP 200 P 3081 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM PP .. |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO CTC PP 3020 Polypropylene Copolymer X-PRO PP 3020 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Nozzle Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO PP 2021 Polypropylene Impact Copolymer X-PRO PP 2021 is an impact, polypropylene copolymer. It has general purpose applications.Data provided by Composite Technologies (CTC). |
|||
Nozzle Temperature | 199 - 216 °C | 390 - 420 °F | |
ExxonMobil Santoprene® 8201-80 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |