Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 275 - 285 °C | 527 - 545 °F | |
Nilit Nilamid A G5 FR PH1 25% Glass Fiber Reinforced, Flame Retardant PA66 Description: Nilamid A G5 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a complete yellow card, with RTI and CTI listings. The formulation has been optim.. |
|||
Nozzle Temperature | 275 - 285 °C | 527 - 545 °F | |
Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optim.. |
|||
Nozzle Temperature | 275 - 285 °C | 527 - 545 °F | |
Nilit Nilamid A G10 FR PH1 50% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous) Description: Nilamid A G10 FR PH1 was developed specifically for highly loaded, structural applications in the electrical industry. It combines extremely high mechanical performance with flame retar.. |
|||
Nozzle Temperature | 275 - 285 °C | 527 - 545 °F | |
Nilit Nilamid A G5 FR C4 25% Glass Fiber Reinforced, Flame Retardant PA66 (with Halogens) Description: Nilamid A G5 FR C4 combines excellent mechanical performance with flame retardancy. The halogenated flame retardant system used in this product allows a wide range of colors. This produ.. |
|||
Nozzle Temperature | 275 - 290 °C | 527 - 554 °F | |
Nilit Nilamid A3 H ZC High Impact PA66 Description: Nilamid A3 H ZC has outstanding impact performance, even at minus temperatures. It is widely used for components subjected to high shock loads. Applications include bicycle components, .. |
|||
Nozzle Temperature | 275 - 290 °C | 527 - 554 °F | |
Nilit Nilamid A3 H ZE High Impact PA66 Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength.. |
|||
Nozzle Temperature | 275 °C | 527 °F | Nozzle (Melt) |
ExxonMobil Escorene® HD-6908 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Excellent Stiffness, Good ImpactUses: Crates, Pails, Industrial containers |
|||
Nozzle Temperature | 275 °C | 527 °F | Average value: 275 °C Grade Count:5 |
Overview of materials for EMAAA Terpolymer This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Nozzle Temperature | 275 °C | 527 °F | Die |
DuPont Bynel® E403 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Nozzle Temperature | 275 - 320 °C | 527 - 608 °F | |
LG Chemical LUCON CP-4201F Conductive Thermoplastic, Flame Retardant LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Nozzle Temperature | 275 - 290 °C | 527 - 554 °F | |
Lavergne VYPET VNT 230 PET - PBT 30% Glass Reinforced Polyester Vypet VNT 230 is a 30% fiberglass reinforced modified PBT/PET polyester injection molding compound designed for electrical applications requiring improved surface aesthetics and improved UV resistan.. |
|||
Nozzle Temperature | 275 - 290 °C | 527 - 554 °F | |
Lavergne VYPET VNT 245 PET - PBT 45% Glass Reinforced Polyester Vypet VNT 245 is a 45% fiberglass reinforced modified PBT / PET polyester injection molding compound designed for electrical and automotive applications requiring low warp and improved surface finis.. |
|||
Nozzle Temperature | 275 - 290 °C | 527 - 554 °F | |
Lavergne VYPET VNT 325 PET 25% Glass - Mineral Reinforced Vypet 325 is a 25% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Good balance resilience-stiffne.. |
|||
Nozzle Temperature | 275 - 300 °C | 527 - 572 °F | |
Lavergne VYPET VNT 335 PET 35% Glass - Mineral Reinforced Vypet VNT 335 is a 35% glass/mineral reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityT.. |
|||
Nozzle Temperature | 275 - 300 °C | 527 - 572 °F | |
Lavergne VYPET VNT 340 PET 40% Glass - Mineral Reinforced Vypet VNT 340 is a 40% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications, with High Dielectric StrengthFeatures: High temperature performanc.. |
|||
Nozzle Temperature | 275 - 295 °C | 527 - 563 °F | |
Lavergne VYPET VNT 615 FR PET 15% Glass Reinforced, Flame Retardant Vypet VNT 615 FR is a 15% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216.. |
|||
Nozzle Temperature | 275 - 295 °C | 527 - 563 °F | |
Lavergne VYPET VNT 615 HP PET 15% Glass Reinforced Vypet VNT 615HP is a modified 15% fiberglass reinforced PET injection molding compound designed for automotive structural applications.Features: Easy, fast processing; Excellent strength and stiffne.. |
|||
Nozzle Temperature | 275 - 300 °C | 527 - 572 °F | |
Lavergne VYPET VNT 645 PET 45% Glass Reinforced Vypet VNT 645 is a 45% glass reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Excellent strength and stiffness; E.. |
|||
Nozzle Temperature | 275 - 300 °C | 527 - 572 °F | |
Lavergne VYPET VNT 835 PET 35% Glass-Mineral Reinforced Vypet VNT 835 is a 35% mineral and fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional s.. |
|||
Nozzle Temperature | 275 - 300 °C | 527 - 572 °F | |
Lavergne VYPET VNT 840 HY PET 40% Glass-Mineral Reinforced Vypet VNT 840 HY is a 40% glass/mineral reinforced PET high strength injection molding compound with improved hydrolysis stability designed for electrical and structural applications, with High Diel.. |
|||
Nozzle Temperature | 275 - 280 °C | 527 - 536 °F | |
Lavergne VYTEEN PC/ABS 8515XF Polycarbonate - Acrylonitrile Butadiene Styrene Alloy Vyteen PC/ABS 8515XF is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High d.. |
|||
Nozzle Temperature | 275 - 300 °C | 527 - 572 °F | |
Lavergne VYPET VNT 615 PET 15% Glass Reinforced Vypet VNT 615 is a 15% fiberglass reinforced PET injection molding compound designed for structural applications.Features: Easy, fast processing; Excellent strength and stiffness; Excellent dimensio.. |
|||
Nozzle Temperature | 275 °C | 527 °F | Die |
DuPont Bynel® 2022 Acid-Modified Ethylene Terpolymer Adhesive Resin Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Nozzle Temperature | 275 °C | 527 °F | |
Beijing Chemical Industry KAIFA® M104N MPPO Resin High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 275 °C | 527 °F | |
Beijing Chemical Industry KAIFA® M104 MPPO Resin Flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 275 °C | 527 °F | |
Beijing Chemical Industry KAIFA® M106N MPPO Resin High Flame retardant, High thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 275 °C | 527 °F | Die |
DuPont Bynel® 20E482 Acid-Modified Ethylene Terpolymer Adhesive Resin
(discontinued **) Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature .. |
|||
Nozzle Temperature | 275 - 320 °C | 527 - 608 °F | |
LG Chemical LUCON CP-4208F Conductive Thermoplastic, Flame Retardant LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |