Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
Nilit Polynil® N66-P300 High Viscosity Nylon 6/6 Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-100L Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-G13HL 13% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-G13L 13% Glass Fiber Reinforced Lubed Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-G33 33% Glass Fiber Reinforced Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-T100 Toughened Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Tristar® PC-10R-(V15) 15 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Tristar® PC-10R-CL(15) 15 MFI Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Tristar® PC-10R-CL(V15) 15 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
Oxford Polymers PC C20-000 Clear PC Product Description: Amorphous, Unreinforced Polycarbonate injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Pigment onlySpecial Characteristics: Easy fl.. |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Trimid® N66-G13LU 13% Glass Fiber Reinforced Utility Lubricated Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Tristar® PC-10FR-(16) 16 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Tristar® PC-10FR-(V16) 16 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
PTS Tristar® PC-15R-113 15 MFI Clear Utility Grade Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
Mitsubishi Iupilon® S3000R 16.5 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
Mitsubishi Iupilon® S3000UR 16.5 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 282 °C | 510 - 540 °F | |
Mitsubishi Iupilon® S3001R 16.5 MFI FDA Compliant Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman EcoLon® 2000-BK1 37% Post Consumer Compound Nylon 66 Description: Post Consumer Compound Nylon 66Information provided by Wellman. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® 220-N Unfilled Nylon 66, Not Lubricated, Nucleated, or Heat Stabilized Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® 22LHI4 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® 22LH-N Unfilled Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® 22LN2-N Unfilled Nylon 66, Lubricated & Nucleated Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® MRGF25/15 22H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66 Description: Medium Impact Nylon 66Information provided by Wellman. |
|||
Nozzle Temperature | 266 - 277 °C | 510 - 530 °F | |
Entec Hylex® P1317FR Polycarbonate Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Nozzle Temperature | 266 - 271 °C | 510 - 520 °F | |
Diamond Polymers ASA M-523 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Nozzle Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant Renol PA611D40 Nylon 612, Glass Fiber Reinforced, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Nozzle Temperature | 266 - 271 °C | 510 - 520 °F | |
Diamond Polymers ASA M-143 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |