Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 230 °C | 446 °F | |
Inchem Phenoxy PKFE Phenoxy PKFE - polyhydroxy ether of Bisphenol A. Originally developed by Union Carbide. Produced by InChem Corporation. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT 1068D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT HB9242D Ester Type TPE Description: TPC-ET, Blow Moldable, Low Modulus, Black ColorApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUMAX HF-5006F High Flow PBT, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUMAX IN-5001 High Impact PBT LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical LUMIPLAS LD590 Light diffusion ABS Description: Injection Molding, Light diffusion, Medium ImpactApplication: (LED) Lamp Cover, Signboard Lighting Decoration of Electronic DeviceCAS No. 9010-94-0Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUPOS GP2205 SAN+GF20%, General Purpose Feature: Injection Molding, SAN+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUPOS GP2206F ABS+GF20%, Flame Retardant Feature: Injection Molding, ABS+GF20%, Flame RetardantApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7, 65997-17-3, 88497-56-7 and 1309-64-4Information provided b.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by .. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR404 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Inf.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay TECHNYL® C 218 V 50 PA6, 50% glass fiber, Eh 0 Description: TECHNYL C 218 V50 is a polyamide 6 reinforced with 50% of glass fiber with excellent thermal stabilityColors: it is supplied in natural color and black color.Available in: Latin America.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
Stellarchem SE/PA745B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® WR-9330I Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | |
Samyang Tribit® 1503 Polybutylene Terephthalate Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
Unitika AX-1500W Conditioned Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
Unitika AX-1500W Dry Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | |
Unitika A1030JR PA6, Dry Information provided by Unitika Ltd. |
|||
Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
Arkema Group Pebax® 7033 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Nozzle Temperature | 230 - 290 °C | 446 - 554 °F | |
Arkema Group Pebax® Rnew 63R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 63R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Nozzle Temperature | 230 - 255 °C | 446 - 491 °F | Injection Molding |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Nozzle Temperature | 230 - 305 °C | 446 - 581 °F | Average value: 279 °C Grade Count:10 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an.. |
|||
Nozzle Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT S5035 Ester Type TPE Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide.. |
|||
Nozzle Temperature | 230 - 240 °C | 446 - 464 °F | Injection Molding |
LG Chemical XR401F ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (MWO Door Frame)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG Chemical |
|||
Nozzle Temperature | 230 °C | 446 °F | Typical Die Temp. |
DuPont Nucrel® 1214 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating