Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products CC40P100-00EG 40% Calcium Carbonate Reinforced Polypropylene, Natural, Extrusion Grade Applications: Consumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products F37-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: ElectronicsBracketsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products F40-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysAir cleaner housingFunctional support decksInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products F55-01 43% Glass Fiber/Talc Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Consumer goodsSupportsGolf cart bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products G40P100-00 40% Glass Fiber Reinforced Polypropylene, Natural Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products G40P100-01 40% Glass Fiber Reinforced Polypropylene, Black Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products G40P100-04UV 40% Glass Fiber Reinforced Polypropylene, UV Stabilized, White Injection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products GC40P100-00 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products GC40P100-01 40% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products GC43P250-777 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Ivory Applications: BracketsStructural supportsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 441 - 460 °F | |
PolyOne OnFlex™ HFFR 360-0185 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 360-0185 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - Non-halogen flame re.. |
|||
Nozzle Temperature | 227 - 238 °C | 441 - 460 °F | |
PolyOne OnFlex™ HFFR 361-0190 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 361-0190 is a non-halogen flame retardant material designed for injection molding applications. New Product. Commercial specifications have not been established. - UL 94 HB compliantPu.. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products M40P100-01 40% Mica Reinforced Polypropylene, Black Applications: Structural componentsAir ducts and dampenersFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products M40P200-01 40% Mica Reinforced Polypropylene Copolymer, Black Applications: Automotive applicationsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products RCT140-01A 40% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC ductworkI/P componentsFuse panel assembliesUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P100-01 40% Talc Reinforced Polypropylene, Black Applications: Wire troughBracketsConsolesFan shroudsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P105-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P105-04 40% Talc Reinforced Polypropylene, White, 5% Titanium Dioxide Applications: Instrument cluster masksAutomotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P106-01 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 238 °C | 440 - 460 °F | |
RheTech Products T40P250-00 40% Talc Reinforced Polypropylene Copolymer, Natural Applications: BracketsHousingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Nozzle Temperature | 227 - 293 °C | 440 - 560 °F | |
Wellman Wellamid® 42LH XE-N Unfilled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Automotive seat belt, buckle and anchor components; convoluted tubing for wire harnesses; furniture hardware, curtain glides.Data provided by the manufacturer, Wellman Inc. |
|||
Nozzle Temperature | 227 °C | 441 °F | |
Lubrizol ESTAGRIP® ST70A Polyether-Type Thermoplastic Polyurethane Features: Low durometer soft feel for excellent grip; outstanding adhesionUses: Injection Molding - OvermoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation provided.. |
|||
Nozzle Temperature | 227 °C | 441 °F | |
Lubrizol ESTAGRIP® ST80A Polyether-Type Thermoplastic Polyurethane Features: Low durometer soft feel for excellent grip; outstanding adhesionUses: Injection Molding - OvermoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation provided.. |
|||
Nozzle Temperature | 227 °C | 441 °F | |
Lubrizol ESTALOC® 60204 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Nozzle Temperature | 227 - 277 °C | 440 - 530 °F | |
Elastocon TPE Technologies Elastocon® STK60 Thermoplastic Elastomer Elastocon® STK60 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60 is FDA compliant and well s.. |
|||
Nozzle Temperature | 227 - 277 °C | 440 - 530 °F | |
Elastocon TPE Technologies Elastocon® STK70 Thermoplastic Elastomer Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer.. |
|||
Nozzle Temperature | 227 - 277 °C | 441 - 531 °F | |
Elastocon TPE Technologies Elastocon® STK40 Thermoplastic Elastomer Elastocon® STK40 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40 is well suited for consumer .. |
|||
Nozzle Temperature | 227 - 249 °C | 440 - 480 °F | |
Advanced Polymer Alloys DuraGrip™ 6150 BK Melt Processable Elastomer DuraGrip™ 6150BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6150BK has an excellent
soft touch feel a.. |
|||
Nozzle Temperature | 227 - 249 °C | 440 - 480 °F | |
Advanced Polymer Alloys DuraGrip™ 6160 BK Melt Processable Elastomer DuraGrip™ 6160BK is designed to be a special purpose Melt Processable Elastomer (MPE) that is easy to use in injection molding and extrusion processes. DGR 6160BK has an excellent
soft touch feel a.. |