Processing Properties | Metric | English | Comments |
---|---|---|---|
Cushion | 0.330 - 0.635 cm | 0.130 - 0.250 in | |
MRC Polymers MAXTELâ„¢ 600 GF20 TPO, 20% Glass Fiber Filled For automotive exterior applications. Excellent process ability and dimensional stability.Internal and external lubricants can be addedCan be UV StabilizedInformation provided by MRC Polymers Inc. |
|||
Cushion | 0.330 - 0.635 cm | 0.130 - 0.250 in | |
MRC Polymers MAXTELâ„¢ 600 GF30 TPO, 30% Glass Fiber Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Cushion | 0.330 - 0.635 cm | 0.130 - 0.250 in | |
MRC Polymers NAXALOYâ„¢ 770 ABS + PC Alloy Impact modifiedAvailable in Natural, Black, and GrayCan be Colored (Masterbatch)Low temperature ductility and impact modifiedCan be UV StabilizedInternal and external lubricant can be addedInformati.. |
|||
Cushion | 0.330 - 0.635 cm | 0.130 - 0.250 in | |
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Cushion | 0.330 - 0.635 cm | 0.130 - 0.250 in | |
MRC Polymers NAXALOYâ„¢ 770 GF16 ABS+PC Alloy, 16% Glass Fiber Filled Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Cushion | 0.330 - 0.813 cm | 0.130 - 0.320 in | |
MRC Polymers SATRANâ„¢ 800R ABS Terpolymer, Reprocessed black onlyInformation provided by MRC Polymers Inc. |