Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 50.0 - 150 mm/sec | 1.97 - 5.91 in/sec | Average value: 100 mm/sec Grade Count:7 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Injection Velocity | 50.0 - 150 mm/sec | 1.97 - 5.91 in/sec | Moderate to Fast |
Topas Advanced Polymers TOPAS® 5013L-10 Cyclic Olefin Copolymer (COC) TOPAS® 5013L-10 is a high flow, internally lubricated injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, che.. |
|||
Injection Velocity | 50.0 - 150 mm/sec | 1.97 - 5.91 in/sec | Moderate to Fast |
Topas Advanced Polymers TOPAS® 5013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 5013S-04 is a high flow injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high .. |
|||
Injection Velocity | 50.0 - 150 mm/sec | 1.97 - 5.91 in/sec | Moderate to Fast |
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,.. |
|||
Injection Velocity | 50.0 - 150 mm/sec | 1.97 - 5.91 in/sec | Moderate to Fast |
Topas Advanced Polymers TOPAS® 6015S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6015S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Injection Velocity | 50.0 - 150 mm/sec | 1.97 - 5.91 in/sec | Moderate to Fast |
Topas Advanced Polymers TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6017S-04 is an injection molding grade with a high heat distortion temperature (170°C) and exceptional dimensional stability. It is a glass-clear amorphous polymer with outstanding moisture.. |
|||
Injection Velocity | 50.0 - 150 mm/sec | 1.97 - 5.91 in/sec | Moderate to Fast |
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Injection Velocity | 50.0 - 150 mm/sec | 1.97 - 5.91 in/sec | Moderate to Fast |
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC) TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist.. |