Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 1667 - 3333 mm/sec | 65.63 - 131.2 in/sec | |
Borealis Xmod™ GD301FE Polypropylene, Glass Fiber Reinforced Xmod™ GD301FE is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also a.. |
|||
Injection Velocity | 1667 - 3333 mm/sec | 65.63 - 131.2 in/sec | |
Borealis Xmod™ GB306SAF Polypropylene, Glass Fiber Reinforced Xmod™ GB306SAF is a 35 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. The product is available in standard black 9502. This mat.. |