Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Borcom™ WG140AI Polypropylene Borcom™ WG140AI is a polypropylene microcomposite intended for injection molding. This material has an excellent balance between impact strength and stiffness, high melt flow rate and gives a good.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE PAE1200U Nylon Elastomer Description: UBESTA Nylon 12 ElastomerInformation provided by UBE. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ ED230HP Polypropylene TPO Compound Daplen™ ED230HP is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EE188HP Polypropylene TPO Compound Daplen™ EE188HP is a 15% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and g.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EE255AE Polypropylene TPO Compound Daplen™ EE255AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EF210AE Polypropylene TPO Compound Daplen™ EF210AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EF341AE Polypropylene TPO Compound Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EG250AI Polypropylene TPO Compound Daplen™ EG250AI is a 20% mineral reinforced impact modified polypropylene compound suitable for injection molding. This material has an excellent balance between impact strength and stiffness, giv.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ KB4436 Polypropylene TPO Compound Daplen™ KB4436 is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gi.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3020GX6 Glass Fiber Reinforced Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, glass fiber reinforced, UV resistanceInformation provided by UBE. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3020LU1X3 Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3020X15 Nylon 12 Thermister Description: UBESTA Nylon 12 ThermisterInformation provided by UBE. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3024NUX Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3030JFX1 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3030JI5L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet SAE J844, DIN73378 HIPHLInformation provided by UBE. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis GB366WG Polypropylene Compound, Glass Fiber Reinforced GB366WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis PS65C40 Polypropylene Compound, Mineral Filled PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® P3014UMX Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EF267AI Polypropylene TPO Compound Daplen™ EF267AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3030UFX1 Rigid Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3030XA Nylon 12 Film Description: UBESTA Nylon 12 FilmInformation provided by UBE. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis ME212U Polypropylene Compound, Mineral Filled ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Xmod™ GD302HP Polypropylene, Glass Fiber Reinforced Xmod™ GD302HP is a 30 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. This material has an excellent balance between impact stre.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EF103AE Polypropylene TPO Compound Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis MB350WG Polypropylene Compound, Mineral Filled MB350WG is a 30% mineral filled polypropylene compound intended for injection molding. This material has a very high impact strength while maintaining good stiffness and is easy to process. Applic.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis ME268Al Polypropylene Compound, Mineral Filled ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |