Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 65.0 mm/sec | 2.56 in/sec | Injection molding |
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Conditioned) Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven.. |
|||
Injection Velocity | 65.0 mm/sec | 2.56 in/sec | Injection molding |
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry) Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven.. |
|||
Injection Velocity | 65.0 mm/sec | 2.56 in/sec | Injection molding |
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Conditioned) Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.. |
|||
Injection Velocity | 65.0 mm/sec | 2.56 in/sec | Injection molding |
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Dry) Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.. |
|||
Injection Velocity | 65.0 mm/sec | 2.56 in/sec | Injection molding |
Styrolution Terblend® N NM-12 ABS/PA6 (Conditioned) Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture.. |
|||
Injection Velocity | 65.0 mm/sec | 2.56 in/sec | Injection molding |
Styrolution Terblend® N NM-12 ABS/PA6 (Dry) Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture.. |
|||
Injection Velocity | 65.0 mm/sec | 2.56 in/sec | Injection molding |
Styrolution Terblend® N NMX04 ABS/PA6 (Conditioned) Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU.. |
|||
Injection Velocity | 65.0 mm/sec | 2.56 in/sec | Injection molding |
Styrolution Terblend® N NMX04 ABS/PA6 (Dry) Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU.. |
|||
Injection Velocity | 65.0 mm/sec | 2.56 in/sec | Injection molding |
Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Conditioned) Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.Information provided by STYROLUTION, which is a join.. |
|||
Injection Velocity | 65.0 mm/sec | 2.56 in/sec | Injection molding |
Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Dry) Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.Information provided by STYROLUTION, which is a join.. |
|||
Injection Velocity | 65.0 mm/sec | 2.56 in/sec | Average value: 65.0 mm/sec Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |