Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 13.0 - 25.0 mm/sec | 0.512 - 0.984 in/sec | |
Zhejiang Double Fish YS-G030 30% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Injection Velocity | 13.0 - 25.0 mm/sec | 0.512 - 0.984 in/sec | |
Zhejiang Double Fish YS-G040 40% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Injection Velocity | 13.0 - 25.0 mm/sec | 0.512 - 0.984 in/sec | |
Zhejiang Double Fish YS-G050 50% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |