Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 60.0 - 200 mm/sec | 2.36 - 7.87 in/sec | Average value: 107 mm/sec Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | Average value: 150 mm/sec Grade Count:20 |
Overview of materials for Polypropylene with 20% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Mica Filler". Specific grades with primary filler content between 15% and 24% are.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Borcom™ WE007AE Polypropylene Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ ED230HP Polypropylene TPO Compound Daplen™ ED230HP is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EE108U Polypropylene TPO Compound Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EE168AI Polypropylene TPO Compound Daplen™ EE168AI is a 10% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EE188HP Polypropylene TPO Compound Daplen™ EE188HP is a 15% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and g.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EE340AE Polypropylene TPO Compound Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EF341AE Polypropylene TPO Compound Daplen™ EF341AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EG103AI Polypropylene Compound, Mineral Filled Daplen™ EG103AI is a 15 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and high melt flow rate.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis GB311U Polypropylene Compound, Glass Fiber Reinforced GB311U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis GB364WG Polypropylene Compound, Glass Fiber Reinforced GB364WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis GB366WG Polypropylene Compound, Glass Fiber Reinforced GB366WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis GD310U Polypropylene Compound, Glass Fiber Reinforced GD310U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis HB601WG Polypropylene Homopolymer HB601WG is a polypropylene homopolymer intended for injection molding and blow molding. The product is available in natural but other colors can be provided on request. This material has excellent .. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis HK030U Polypropylene Compound HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wit.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis MD441U Polypropylene Compound, Mineral Filled MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis ME266U Polypropylene Compound, Mineral Filled ME266U is a 20% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and gives a good surface quality. .. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis MG302Al Polypropylene Compound, Mineral Filled MG302AI is a 30% mineral filled polypropylene compound intended for injection and back injection molding. This material has an excellent balance between impact strength and stiffness and high melt .. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis PS65C40 Polypropylene Compound, Mineral Filled PS65C40 is a 40% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives a good surface quality and.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EE065AI Polypropylene Elastomer Modified Daplen™ EE065AI is an elastomer modified polypropylene with increased crystallinity. This material has an excellent balance between impact strength and stiffness. The product is available in natu.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EE188AI Polypropylene TPO Compound Daplen™ EE188AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EE189AI Polypropylene TPO Compound Daplen™ EE189AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EF261AI Polypropylene TPO Compound Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis MS64T20 Polypropylene Compound, Mineral Filled MS64T20 is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: automotive p.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EF103AE Polypropylene TPO Compound Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis MB350WG Polypropylene Compound, Mineral Filled MB350WG is a 30% mineral filled polypropylene compound intended for injection molding. This material has a very high impact strength while maintaining good stiffness and is easy to process. Applic.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis MD231U Polypropylene Compound, Mineral Filled MD231U is a 20 % mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: Air duc.. |