Processing Properties Metric English Comments
Injection Velocity 65.0 mm/sec
2.56 in/sec
Injection molding
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Conditioned)
Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven..
Injection Velocity 65.0 mm/sec
2.56 in/sec
Injection molding
Styrolution Terblend® N NG-04 20% Glass Filled ABS/PA6 (Dry)
Terblend N NG-04 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, low mold shrinkage and high heat resistance.Information provided by STYROLUTION, which is a joint ven..
Injection Velocity 65.0 mm/sec
2.56 in/sec
Injection molding
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Conditioned)
Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS..
Injection Velocity 65.0 mm/sec
2.56 in/sec
Injection molding
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Dry)
Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS..
Injection Velocity 65.0 mm/sec
2.56 in/sec
Injection molding
Styrolution Terblend® N NM-12 ABS/PA6 (Conditioned)
Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture..
Injection Velocity 65.0 mm/sec
2.56 in/sec
Injection molding
Styrolution Terblend® N NM-12 ABS/PA6 (Dry)
Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture..
Injection Velocity 65.0 mm/sec
2.56 in/sec
Injection molding
Styrolution Terblend® N NMX04 ABS/PA6 (Conditioned)
Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU..
Injection Velocity 65.0 mm/sec
2.56 in/sec
Injection molding
Styrolution Terblend® N NMX04 ABS/PA6 (Dry)
Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU..
Injection Velocity 65.0 mm/sec
2.56 in/sec
Injection molding
Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Conditioned)
Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.Information provided by STYROLUTION, which is a join..
Injection Velocity 65.0 mm/sec
2.56 in/sec
Injection molding
Styrolution Terblend® N NG-02 8% Glass Filled ABS/PA6 (Dry)
Terblend N NG-02 is a glass fibre reinforced ABS/PA6 blend with excellent dimensional stability, high impact strength and good surface appearance.Information provided by STYROLUTION, which is a join..
Injection Velocity 65.0 mm/sec
2.56 in/sec
Average value: 65.0 mm/sec Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced