Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis BF335SA Polypropylene Copolymer BF335SA is a polypropylene copolymer intended for injection molding. This material has a very high impact strength while maintaining good stiffness, gives a good surface quality and is
easy to proc.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Borcom™ WE007AE Polypropylene Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE PAE1200U Nylon Elastomer Description: UBESTA Nylon 12 ElastomerInformation provided by UBE. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ ED117AE Polypropylene TPO Compound Daplen™ ED117AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surfac.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EE108U Polypropylene TPO Compound Daplen™ EE108U is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, gives.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EE188HP Polypropylene TPO Compound Daplen™ EE188HP is a 15% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and g.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EE340AE Polypropylene TPO Compound Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EG250AI Polypropylene TPO Compound Daplen™ EG250AI is a 20% mineral reinforced impact modified polypropylene compound suitable for injection molding. This material has an excellent balance between impact strength and stiffness, giv.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EH104AE Polypropylene TPO Compound Daplen™ EH104AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, high.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis EE002AE Polypropylene Elastomer Modified EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3020LU1X3 Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3024LU Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3030JFX1 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3030JI5L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability (DIN 73378 Nomenclature = PA12 HIPHL)Information provided by U.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis GB364WG Polypropylene Compound, Glass Fiber Reinforced GB364WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis GB366WG Polypropylene Compound, Glass Fiber Reinforced GB366WG is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Th.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis GD310U Polypropylene Compound, Glass Fiber Reinforced GD310U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3030JI9L 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, impact modified and stabilized against weatherability, designed for high burst pressure performance at high temperat.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3030JLX1 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: plasticized, stabilized against weatherability (DIN 73378 Nomenclature = PA12 PHL)Information provided by UBE. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis HF700SA Polypropylene HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3030LUX Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EE188AI Polypropylene TPO Compound Daplen™ EE188AI is a 15% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis Daplen™ EF261AI Polypropylene TPO Compound Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3030UFX1 Rigid Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3035UF Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis ME212U Polypropylene Compound, Mineral Filled ME212U is a 20% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: air ducts, air.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® 3030LUX 8x1 mm Black Automotive Grade Nylon 12 Tube Description: UBE UBESTA® Automotive grade Nylon 12 tubePerformance: rigid, stabilized against weatherability (DIN 73378 Nomenclature = PA12 HL)Information provided by UBE. |
|||
Injection Velocity | 100 - 200 mm/sec | 3.94 - 7.87 in/sec | |
Borealis ME268Al Polypropylene Compound, Mineral Filled ME268AI is a 20% mineral filled polypropylene compound intended for injection molding. Applications: ME268AI has been developed especially for the car industry to be used in automotive interior par.. |
|||
Injection Velocity | 100 mm/sec | 3.94 in/sec | Injection Molding |
UBE UBESTA® P3014U Powder Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |