Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 310 - 332 °C | 590 - 630 °F | |
Polymer Resources PC-FD1-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigm.. |
|||
Front Barrel Temperature | 310 - 332 °C | 590 - 630 °F | |
Polymer Resources PC-FR1A-D Polycarbonate, Flame Retardant, Low Flow Polycarbonate, Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing co.. |
|||
Front Barrel Temperature | 310 - 332 °C | 590 - 630 °F | |
Polymer Resources PC-FR1-D Polycarbonate, Improved Flame Retardant, Low Flow Polycarbonate, Improved Flame Retardant, Low FlowFeatures: • High Impact Resistance • High Viscosity • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal t.. |
|||
Front Barrel Temperature | 310 - 332 °C | 590 - 630 °F | |
Polymer Resources PC-GP1-10TFE Polycarbonate, General Purpose, Wear Resistant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 310 - 332 °C | 590 - 630 °F | |
Polymer Resources PC-GP1-D Polycarbonate, General Purpose, Low Flow Polycarbonate, General Purpose, Low FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/.. |
|||
Front Barrel Temperature | 310 - 332 °C | 590 - 630 °F | |
Polymer Resources PC-GP1-D-[color]-1 Polycarbonate, General Purpose, Low Flow with Mold Release Polycarbonate, General Purpose, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Front Barrel Temperature | 310 - 332 °C | 590 - 630 °F | |
Polymer Resources PC-GP1-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Low Flow Polycarbonate, FDA-compliant Feedstocks, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pro.. |
|||
Front Barrel Temperature | 310 - 332 °C | 590 - 630 °F | |
Polymer Resources PC-GP1-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Low Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Front Barrel Temperature | 310 - 332 °C | 590 - 630 °F | |
Polymer Resources PC-GP3-TFE10 Polycarbonate, 10% PTFE, High Flow, Wear Resistant Polycarbonate, General Purpose, High Flow, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Front Barrel Temperature | 310 - 332 °C | 590 - 630 °F | |
Ravago Manufacturing Americas Hylex® P1007L Polycarbonate Information provided by Ravago |
|||
Front Barrel Temperature | 316 - 332 °C | 601 - 630 °F | |
LNP NORYL® EXCP0111 PPS + Polyphenylene Ether, 42% Glass / Mineral Reinforcement
(discontinued **) For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele.. |
|||
Front Barrel Temperature | 316 - 332 °C | 601 - 630 °F | |
LNP NORYL® EXCP0112 PPS + Polyphenylene Ether, 40% Glass / Mineral Reinforcement
(discontinued **) For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele.. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® A-4160 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4160 HSL resin is a 60% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits high modulus at elevated temperatures, a high heat deflection temperature and exceptional cree.. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
Front Barrel Temperature | 310 - 332 °C | 590 - 630 °F | |
Polymer Resources PC-FD1 Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Low Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Front Barrel Temperature | 310 - 332 °C | 590 - 630 °F | |
LTL Color Compounds ColorFast® PC60 Polycarbonate 6 melt extrusion gradeAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA), 22% Mineral Amodel® A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over.. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Conditioned) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications .. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications .. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Conditioned) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry) Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin.. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA), 30% Glass Fiber (Dry) Amodel® AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel® resin. This grade was developed f.. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |
|||
Front Barrel Temperature | 327 - 332 °C | 621 - 630 °F | |
Solvay Specialty Polymers Amodel® AT-6130 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6130 HS is a 30% glass-reinforced, toughened polyphthalamide (PPA) resin that has more elongation than other 30% glass-reinforced grades of Amodel resin. This grade was developed for autom.. |