Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 204 - 216 °C | 399 - 421 °F | |
PolyOne Dynaflex™ G2730 Thermoplastic Elastomer (TPE) Dynaflex™ G2730 is a soft, easy processing compound. - Excellent Weatherability - High Resilience - Soft, Rubbery FeelColor concentrates with polypropylene, ethylene vinyl acetate, or low density p.. |
|||
Front Barrel Temperature | 204 - 216 °C | 399 - 421 °F | |
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE) Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat .. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Front Barrel Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynaflex™ G7650-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G7680-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G7680-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Front Barrel Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Front Barrel Temperature | 193 - 216 °C | 379 - 421 °F | |
PolyOne Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1001-00 is an easy processing, general purpose material designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypro.. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G7950-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7950-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G7950-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7950-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G7960-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Front Barrel Temperature | 177 - 216 °C | 351 - 421 °F | |
PolyOne Dynaflex™ G2703-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2703-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance and a low coefficient of friction. - Adhesion to Polypropylen.. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G6713C Thermoplastic Elastomer (TPE) Dynaflex™ G6713C is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV Sta.. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G7650-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G7960-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G7980-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7980-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Front Barrel Temperature | 188 - 216 °C | 370 - 421 °F | |
PolyOne Dynaflex™ G7980-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylene - Rubbery Feel - Soft T.. |