Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 321 - 343 °C | 610 - 650 °F | |
Polymer Resources PC-BR1 Polycarbonate, Branched for Extrusion and Blow Molding Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical and thermal te.. |
|||
Front Barrel Temperature | 321 - 343 °C | 610 - 650 °F | |
Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical.. |
|||
Front Barrel Temperature | 321 - 343 °C | 610 - 650 °F | |
Polymer Resources PC-BR1-[color]-5 Polycarbonate, Branched, Food Contact Polycarbonate, Branched for Extrusion and Blow MoldingFeatures: • Ultra High Impact Resistance • Ultra High Viscosity • Food Contact AcceptableProcess: Extrusion/Blow MoldingNotes: All physica.. |