Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 266 - 304 °C | 510 - 580 °F | |
Polymer Resources PPX-GP3-IM Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Front Barrel Temperature | 266 - 304 °C | 510 - 580 °F | |
Polymer Resources PPX-GP3-WR Modified-PPO, Wear Resistant Modified-Polyphenylene Oxide, Wear Resistant, 235F HDTFeatures: • Hydrolytically Stable • Low to No Water Absorption • Good Wear ResistanceProcess: Injection MoldingNotes: All physical, mechan.. |
|||
Front Barrel Temperature | 266 - 304 °C | 510 - 580 °F | |
Polymer Resources PPX-GP8 Modified-PPO, Impact Modified Modified-Polyphenylene Oxide, Impact Modified, 240F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Front Barrel Temperature | 266 - 288 °C | 510 - 550 °F | |
MRC Polymers MAXNITE™ 500 GF15 PET, 15% Glass Fiber Filled
(discontinued **) Information provided by MRC Polymers Inc. |
|||
Front Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Firestone CG430-001 Nylon 6, 30% Fiberglass Filled Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone |
|||
Front Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Firestone CG430-203 Nylon 6, 30% Fiberglass Filled Natural color. Heat stabilized. Fiber size is 4 mm length and 14 µm diameter.Information provided by Firestone |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled 13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Wellman EcoLon® MRGF1616-BK 40% Mineral/Glass Reinforced Post Consumer Compound Nylon 6 Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 6Information provided by Wellman. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® 220-N Unfilled Nylon 66, Not Lubricated, Nucleated, or Heat Stabilized Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® 22LHI3 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® 22LHI4 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® 22LHI6 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® 22L-N Unfilled Nylon 66, Lubricated Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® MR340 42H-N 34% Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® MR410 42H-N 40% Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Wellman Wellamid® MRGF25/15 42H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Wellman Wellamid® MRGF30/10 42H-N 30% Mineral/10% Glass Fiber Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® T423-BK10 Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® XT1482-BK High Impact Nylon 66 Description: High Impact Nylon 66Information provided by Wellman. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66 Description: Medium Impact Nylon 66Information provided by Wellman. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® XT1486-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Front Barrel Temperature | 266 - 271 °C | 510 - 520 °F | |
Diamond Polymers ASA M-523 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant 6602-L BK-02 Nylon 66, Lubricated, Nucleated, Weather Resistant, Black Data provided by Clariant Masterbatches |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant 6618G15 HSL UV Black Nylon 66, 15% Glass Fiber, Impact Modified, UV and Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened Data provided by Clariant Masterbatches |
|||
Front Barrel Temperature | 266 - 277 °C | 510 - 530 °F | |
Elastocon TPE Technologies Elastocon® STK56PA-B Thermoplastic Elastomer Elastocon® STK56PA-B black thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK56PA-B is well suited for .. |
|||
Front Barrel Temperature | 266 - 271 °C | 510 - 520 °F | |
Diamond Polymers ASA M-143 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
LTL Color Compounds ColorFast® NY1 Nylon 6 Injection molding nylon 6, with or without lubeAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
LTL Color Compounds ColorFast® NY1GF130 Nylon 6, 13% Glass-Filled 13% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |