Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 250 °C | 482 °F | |
NYCOA 1637 PA 6 plasticized and heat stabilized extrusion grade for the wire jacketing industry to 7,000+ fpm. UL Flammability Component listing for use as cable jacketing.Information provided by NYCOA, Inc. |
|||
Front Barrel Temperature | 250 °C | 482 °F | |
NYCOA 1838 Copolymer Nylon Alloy good impact resistant molding and extrusion gradeInformation provided by NYCOA, Inc. |
|||
Front Barrel Temperature | 250 °C | 482 °F | |
NYCOA 2025 Nylon 6 extrusion and molding grade with mold release and quicker cycle times for sports cleatsInformation provided by NYCOA, Inc. |
|||
Front Barrel Temperature | 250 °C | 482 °F | |
NYCOA 2237 Copolymer Nylon 6/66 Alloy transparent molding and extrusion gradeInformation provided by NYCOA, Inc. |
|||
Front Barrel Temperature | 250 °C | 482 °F | |
NYCOA 27/300I Glass Filled Nylon 6 30% glass filled, flame retardant to UL 94 V-0 nylon 6Information provided by NYCOA, Inc. |
|||
Front Barrel Temperature | 250 °C | 482 °F | |
NYCOA 27/330KNF Glass Filled Nylon 6 33% glass filled, heat stabilized nylon 6Information provided by NYCOA, Inc. |
|||
Front Barrel Temperature | 250 °C | 482 °F | |
NYCOA 27/440KNF Glass Filled Nylon 6 44% glass filled, heat stabilized nylon 6Information provided by NYCOA, Inc. |
|||
Front Barrel Temperature | 250 °C | 482 °F | |
NYCOA 567 PA 6 plasticized general purpose molding and extrusion grade used in shoe heels and mono.Information provided by NYCOA, Inc. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Start Point: 260°C |
Kingfa LONOY 1600 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Start Point: 260°C |
Kingfa LONOY 3010 Glass Fiber Reinforced PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingElectric and electronic partsBusiness machine cabinetGarden to.. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GN5008HF PC/ABS, Halogen Free Flame Retardant, High Impact Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: E&E (OA, Navigation Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP5056F PC/ABS+GF5%, Flame Retardance Description: Injection Molding, PC/ABS+GF5%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG .. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP5100 PC/ABS+GF10% Description: Injection Molding, PC/ABS+GF10%, General Purpose, GF ReinforcedApplication: Electrical Appliance Housing, Automotive I/PCAS: 103598-77-2, 9003-56-9 and 65997-17-3Information provided by.. |
|||
Front Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUPOY HP5004 PC/ABS, High Impact at Low Temperature Description: Injection Molding, PC/ABS, General Purpose, High Impact at Low Temperature, High Flow, Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9003-56-9Information provided.. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | |
Lavergne VYTEEN PC/ABS 8515 Polycarbonate - Acrylonitrile Butadiene Styrene Alloy Vyteen PC/ABS 8515 is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High def.. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP1000MR PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, Mold ReleaseApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Front Barrel Temperature | 250 - 280 °C | 482 - 536 °F | |
Teknor Apex Beetle® PBTC115F Polybutylene Terephthalate and Polyethylene Terephthalate Notes: PBTC115F is a 15% glass fiber reinforced PBT/PET alloy. It provides a good balance of mechanical performance and thermal endurance with excellent surface finish and mold release. Features: G.. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | |
Unitika AX-1500 Conditioned AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | |
Unitika AX-1500 Dry AX series resins are opaque polymer alloys with a high deflection temperature under load without reinforcement and a chemical resistance as high as those of crystalline resins. They are excellent in.. |
|||
Front Barrel Temperature | 250 °C | 482 °F | For high temperature coextrusions. |
DuPont Bynel® 41E687 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Front Barrel Temperature | 250 °C | 482 °F | Cast film |
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent .. |
|||
Front Barrel Temperature | 250 °C | 482 °F | Cast film |
DuPont Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer Elvaloy® 1820 AC is intended for film coextrusion, compounding and injection molding. Due to its high melt flow rate, it also can be used in extrusion coating/lamination. Elvaloy® 1820 AC has go.. |
|||
Front Barrel Temperature | 250 °C | 482 °F | Cast film |
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Front Barrel Temperature | 250 °C | 482 °F | Cast film |
DuPont Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer Elvaloy® 1218 AC is intended for coextrusion, compounding and injection molding. Elvaloy® 1218 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent sealing pro.. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Zone 3 |
Eurostar Starflam PK0022E PA6, 10% Mineral Filled, Injection Molded PK0022E is a Halogen Free and Phosphorous Free, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3620Z22 or PA 10E6 U9 Z22)Information provided by Polymer Technology & Services, the Nor.. |
|||
Front Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Zone 3 |
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
Front Barrel Temperature | 250 °C | 482 °F | Cast film |
DuPont Elvaloy® 3107 AC Ethylene and 7% Butyl Acrylate Copolymer
(discontinued **) Elvaloy® 3107 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3107 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag.. |
|||
Front Barrel Temperature | 250 - 265 °C | 482 - 509 °F | Injection Molding |
LG Chemical LUPOY GP1000ML PC, Transparent Description: Injection Molding, PC, General Purpose, TransparencyApplication: IT/OA Housing and Components, Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Front Barrel Temperature | 250 °C | 482 °F | Cast film |
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |
|||
Front Barrel Temperature | 250 °C | 482 °F | Cast film |
DuPont Elvaloy® 3108 AC Ethylene and 7% Butyl Acrylate Copolymer
(discontinued **) Elvaloy® 3108 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3108 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag.. |