Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 1004 R Polypropylene Features: Scratch Resistance, GoodHeat Resistance, HighStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Front Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 2004 R Polypropylene Glass Fiber Reinforced, 20% by weight.Features:Heat Resistance, HighScratch ResistantStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided .. |
|||
Front Barrel Temperature | 216 - 260 °C | 420 - 500 °F | |
Multibase Multi-Pro® 3012 RC Polypropylene Glass Fiber Reinforced, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products F15-01 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: HousingsBattery traysInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products FT7012-707UV Thermoplastic Polyolefin, UV Stabilized, 848 Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products FT7013-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesLift gate coversI/P componentsClose-out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products FT7016-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products FT7016-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products GC30P103-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: Battery traysFender apronsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products GC30P104-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products GC30P105-08FA 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black Applications: Water system housingFDA approved partsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products GC30P200-00 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products GC30P200-01UV 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black Applications: Interior componentsStructural housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T28P100-01EG 28% Talc Reinforced Polypropylene, Black, Extrusion Grade Applications: Window trimConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products T30P200-01BG 30% Talc Reinforced Polypropylene Copolymer, Black, Blow Molding Grade Applications: HVAC ductsSeat backsFlipper panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LGF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 30% long glass fiber reinforcementInformation provided by Plas.. |
|||
Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
Polymer Resources ABS-GP1-[color]-EP General Purpose ABS, Electroplating Grade General Purpose Acrylonitrile Butadiene Styrene, Electroplating GradeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Front Barrel Temperature | 216 - 235 °C | 420 - 455 °F | |
Ravago Manufacturing Americas Hylac® HF143 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products F15-00UV 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV-Stabilized, Natural Applications: Functional SupportsElectrical housingsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products G30P100-00 30% Glass Fiber Reinforced Polypropylene, Natural Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LCF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LGF20 - TPU Rigid Thermoplastic Polyurethane, 20% Long Glass Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyurethane with 20% long glass fiber reinforcementInformation provided by PlastiComp, Inc.. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products HP525-283 30% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, RK8 Medium Camel Applications: Automotive interior applicationsFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
PlastiComp Complet® LGF50 - TPU Rigid Thermoplastic Polyurethane, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 50% long glass fiber reinforcementInformation provided by Plas.. |
|||
Front Barrel Temperature | 216 - 266 °C | 420 - 510 °F | |
Elastocon TPE Technologies Elastocon® STK60 Thermoplastic Elastomer Elastocon® STK60 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60 is FDA compliant and well s.. |
|||
Front Barrel Temperature | 216 - 266 °C | 420 - 510 °F | |
Elastocon TPE Technologies Elastocon® STK40B Thermoplastic Elastomer Elastocon® STK40B is a black thermoplastic elastomer that has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40B is well s.. |
|||
Front Barrel Temperature | 216 - 227 °C | 420 - 440 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6030 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6030 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6030 NC/BK have
an excellent soft t.. |
|||
Front Barrel Temperature | 216 - 243 °C | 420 - 470 °F | |
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 216 - 238 °C | 420 - 460 °F | |
LTL Color Compounds ColorFast® GPA300X ABS Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc. |