Polymer Property : Front Barrel Temperature = 241 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature >= 116 °C
>= 241 °F
Borealis Polycure™ PC780 Flame Retardant Crosslinking Polyethylene Compound for Low Voltage Insulation
Polycure PC780 is a natural, chemically crosslinking polyethylene compound designed for flame retardant low voltage wire insulation and jacketing. PC780 contains a halogen-based, flame retardant ad..