Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-GP4-[color]-1 Polycarbonate, General Purpose, Easy Flow with Mold Release Polycarbonate, General Purpose, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-GP4-[color]-4 Polycarbonate, UV-stabilized, Easy Flow with Mold Release Polycarbonate, UV-stabilized, Easy Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-GP4-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Easy Flow Polycarbonate, FDA-compliant Feedstocks, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
PTS Tristar® PC-10R-(14) 14 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
PTS Tristar® PC-10R-(VE) 12 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 277 - 293 °C | 531 - 559 °F | |
PolyOne Stat-Tech™ OC-0307081 Black Acrylonitrile Butadiene Styrene + PC (ABS+PC) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Polymer Resources PC-UV4 Polycarbonate, UV-stabilized, Easy Flow Polycarbonate, UV-stabilized, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
PTS Tristar® PC-10FR-(V) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
PTS Tristar® PC-10FR-(VIM) 12 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
PTS Tristar® PC-10FRN 15 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
PTS Tristar® PC-10FRNH-V 12 MFI Non-Bromine Non-Chlorine Flame Retardant UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
LTL Color Compounds ColorFast® NY2GF130 Nylon 66, 13% Glass-Filled 13% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
LTL Color Compounds ColorFast® NY2GF131 Nylon 66, 13% Glass-Filled, Impact Modified 13% glass-filled impact modified nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
LTL Color Compounds ColorFast® NY2GF330 Nylon 66, 33% Glass-Filled 33% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
MRC Polymers EMAREXâ„¢ 300 GF43 Nylon 6, 43% Glass Fiber Filled Available in Black onlyCan be UV and Heat StabilizedProperty data for DAM samples.Information provided by MRC Polymers Inc. |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
MRC Polymers NAXELLâ„¢ PC23M-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Low Viscosity Can be impact modifiedInternal and external lubricant can be addedBlack onlyInformation provided by MRC Polymers Inc. |
|||
Front Barrel Temperature | 282 - 293 °C | 540 - 560 °F | |
MRC Polymers NAXELLâ„¢ PC429HHI Polycarbonate, Impact Modified, High MFR, EZ Flow Good Property RetentionHeat and Dimensional StabilityHigh Melt Impact ModifiedMFR can be modified between 10 to 26 g/10minsCan be UV stabilizedGenerally for natural, colorable and can go blackIntern.. |
|||
Front Barrel Temperature | 277 - 293 °C | 530 - 560 °F | |
Samyang Trirex® PC-3025U 12 MFI UV Stabilized Clear Polycarbonate Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Wellman EcoLon® MR1660-BK 40% Mineral Reinforced Post Consumer Compound Nylon 66 Description: Mineral Reinforced Post Consumer Compound Nylon 66Information provided by Wellman. |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Wellman Wellamid® MR259 22LH-N 25% Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 271 - 293 °C | 520 - 560 °F | |
Wellman Wellamid® MRT1487-N Mineral Reinforced Nylon 66, Lubricated & Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Front Barrel Temperature | 260 - 293 °C | 500 - 560 °F | |
Clariant 66G43HLS-Black Nylon 66, 43% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened Data provided by Clariant Masterbatches |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
LTL Color Compounds ColorFast® NY1 Nylon 6 Injection molding nylon 6, with or without lubeAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
LTL Color Compounds ColorFast® NY1GF130 Nylon 6, 13% Glass-Filled 13% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled 33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 266 - 293 °C | 510 - 560 °F | |
LTL Color Compounds ColorFast® NY2 Nylon 66 Nylon 6,6 with or without lubeAll information provided by LTL Color Compounders, Inc. |