Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 277 - 282 °C | 530 - 540 °F | |
Polymer Resources NY66-EX1 High Viscosity Nylon 66 Nylon 66, High Viscosity (RV 220 to 260)Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as .. |
|||
Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Polymer Resources NY66-IMG33 Nylon, 33% Glass Reinforced, Impact Modified (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-FR2 Flame Retardant PC/Polyester Alloy Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p.. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-GP2-[color]-UV PC/Polyester Alloy, UV-stabilized High Impact, Excellent Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-GP3-G10 PC/Polyester Alloy, 10% Glass Reinforced Superior Chemical Resistance, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Front Barrel Temperature | 243 - 282 °C | 470 - 540 °F | |
Polymer Resources PPX-MF-FR1 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha.. |
|||
Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Ravago Manufacturing Americas Hylex® P1018LLT Polycarbonate Information provided by Ravago. |
|||
Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced Information provided by Ravago. |
|||
Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Ravago Manufacturing Americas Hylex® P1318LLT Polycarbonate Information provided by Ravago. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-GP1 PC/Polyester Alloy High Impact, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Pol.. |
|||
Front Barrel Temperature | 257 - 282 °C | 495 - 540 °F | |
Star Plastics PC/PET7901 Molding Grade PC/PET Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 263 - 282 °C | 505 - 540 °F | |
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by.. |
|||
Front Barrel Temperature | 263 - 282 °C | 505 - 540 °F | |
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Front Barrel Temperature | 263 - 282 °C | 505 - 540 °F | |
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade Notes: Medium-Impact; General Purpose; Impact modified to provide excellent toughness Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS-DB41 CPN3992 Color: W.. |
|||
Front Barrel Temperature | 263 - 282 °C | 505 - 540 °F | |
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St.. |
|||
Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Wellman EcoLon® MRGF1518-BK Mineral/Glass Fiber Reinforced Nylon 66, Lubricated, Heat Stabilized, PCR Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® 22LHI4 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® 22LH-N Unfilled Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® 22LN2-N Unfilled Nylon 66, Lubricated & Nucleated Typical Applications: Automotive components, gears, switches, bearings, pulleys, fasteners, electrical coil forms, chain-saw hand guards, cable ties, furniture hardware, small appliance housings, ae.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® MR410 42H-N 40% Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Wellman Wellamid® MRGF3822-BK 38% Mineral/10% Glass Fiber Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® T423-BK10 Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® XT1482-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® XT1486-BK Medium Impact Nylon 66 Description: Medium Impact Nylon 66Information provided by Wellman. |
|||
Front Barrel Temperature | 266 - 282 °C | 510 - 540 °F | |
Wellman Wellamid® XT1486-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Entec Hylex® P1317FR Polycarbonate Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Front Barrel Temperature | 271 - 282 °C | 520 - 540 °F | |
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Front Barrel Temperature | 268 - 282 °C | 515 - 540 °F | |
Teknor Apex Chemlon® 133 G Nylon 66, 33% Short Glass Fiber Filled Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex |
|||
Front Barrel Temperature | 263 - 282 °C | 505 - 540 °F | |
Teknor Apex Chemlon® 140 MH Nylon 66, 40% Mineral Reinforced Notes: 40% Mineral; High rigidity with exceptional control of warpage and surface sink marks; Excellent for large parts; Fast cycling Features: Fast Molding Cycle; High Rigidity; Heat Stabilized; Lo.. |