Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-FR IM PBT, Impact Modified, Flame Retardant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-FRHG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame Retardant Polybutylene Terephthalate, 15% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-FV699 PBT, 10% Glass Reinforced Structural Foam Grade, Low Shrinkage Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-G10 Polybutylene Terephthalate, 10% Glass Reinforced Polybutylene Terephthalate, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-G15 Polybutylene Terephthalate, 15% Glass Reinforced Polybutylene Terephthalate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-G20 Polybutylene Terephthalate, 20% Glass Reinforced Polybutylene Terephthalate, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Front Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
Polymer Resources TP-GFMF1 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame Retardant Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-HG15 Polybutylene Terephthalate, 15% Glass Reinforced Alloy Polybutylene Terephthalate, 15% Glass Reinforced AlloyProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informatio.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-IM-G15 Polybutylene Terephthalate, 15% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 15% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TP-IM-G30 Polybutylene Terephthalate, 30% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 30% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Front Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
Polymer Resources TP-M30 Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced Warpage Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TPSF-FRG10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced, Flame RetardantProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TPSF-G30 Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 30% Glass Reinforced Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Front Barrel Temperature | 238 - 266 °C | 460 - 510 °F | |
PTS Trimid® N6-615I-NC Extrusion Grade Nylon 6 Total Extractables < 1.5.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 238 - 266 °C | 460 - 510 °F | |
PTS Trimid® N6-G15L 15% GFR Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 511 °F | |
LNP VALOX® SMV5845 PBT + PET Alloy, 16% Carbon Fiber Reinforcement
(discontinued **) ESD Applications. Will be VC1600.Features: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.Th.. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 511 °F | |
LNP VALOX® SMV5846 PBT + PET Alloy, 20% Carbon Fiber Reinforcement
(discontinued **) ESD ApplicationsFeatures: Good Chemical Resistance, High Flow, Flame RetardantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is .. |
|||
Front Barrel Temperature | 232 - 266 °C | 450 - 511 °F | Injection Molding |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (DAM) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Front Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
MRC Polymers NAXALOYâ„¢ 780 PC+PBT Polyester Blend Good chemical resistance, impact and heat resistance.Information provided by MRC Polymers Inc. |
|||
Front Barrel Temperature | 254 - 266 °C | 490 - 510 °F | |
MRC Polymers NAXALOYâ„¢ 793A3 GF10 PC and Polyester Blend, 10% Glass Fiber Filled 793 GF10 is available in natural and custom colors, internal and external lubricants, UV stabilizer and other modifications.Information provided by MRC Polymers Inc. |
|||
Front Barrel Temperature | 246 - 266 °C | 475 - 510 °F | |
Star Plastics PC/PBT7804 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 216 - 266 °C | 420 - 510 °F | |
Elastocon TPE Technologies Elastocon® STK60B Thermoplastic Elastomer Elastocon® STK60B black thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60B is well suited for .. |
|||
Front Barrel Temperature | 216 - 266 °C | 421 - 511 °F | |
Elastocon TPE Technologies Elastocon® STK60X Thermoplastic Elastomer Elastocon® STK60X thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK60X is well suited for consume.. |
|||
Front Barrel Temperature | 216 - 266 °C | 420 - 510 °F | |
Elastocon TPE Technologies Elastocon® STK70 Thermoplastic Elastomer Elastocon® STK70 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK70 is well suited for consumer.. |
|||
Front Barrel Temperature | 216 - 266 °C | 421 - 511 °F | |
Elastocon TPE Technologies Elastocon® STK40 Thermoplastic Elastomer Elastocon® STK40 thermoplastic elastomer has been developed for applications that require ultra soft rubber-like properties and a good surface finish. Elastocon® STK40 is well suited for consumer .. |
|||
Front Barrel Temperature | 249 - 266 °C | 480 - 510 °F | |
Engineered Polymer Solutions PBT VM 450, 20% Mineral Filled Plate-able. Natural and colors available. Injection molding grade. Uses: Automotive, appliancesInformation provided by Engineered Polymer Solutions. |