Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 326 - 339 °C | 619 - 642 °F | |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA), 33% Glass Fiber Amodel® A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment... |
|||
Front Barrel Temperature | 326 - 339 °C | 619 - 642 °F | |
Solvay Specialty Polymers Amodel® AS-1935 HS Polyphthalamide (PPA), 35% Glass Fiber Amodel® AS-1935 HS is a 35% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Front Barrel Temperature | 326 - 339 °C | 619 - 642 °F | |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |