Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 260 - 302 °C | 500 - 575 °F | |
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-GP1-[color]-3 PC Polyester, High Impact, Good Chemical Resistance, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-GP1-UV PC/Polyester Alloy, UV-stabilized High Impact, Good Chemical Resistance, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Front Barrel Temperature | 260 - 282 °C | 500 - 540 °F | |
Polymer Resources PC/TP-GP3-G30 PC/Polyester Alloy, 30% Glass Reinforced Superior Chemical Resistance, 30% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information pr.. |
|||
Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
PTS Tristar® PC-10R-CL(V22) 22 MFI UV Stabilized Clear Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Start Point: 265°C |
Kingfa PA6-MG45 45% Glass & Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
LG Chemical LUMID GP1000B(W) PA66, General Purpose, Low Viscosity Feature: Injection Molding, PA66, General Purpose, Low ViscosityApplication: Buckles, Chair NobCAS No. 32131-17-2Information provided by LG Chemical |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
Front Barrel Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
LG Chemical LUPOY GN5151RFA PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9, 181028-79-5 an.. |
|||
Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
Mitsubishi Iupilon® H2000UR 23 MFI, UV Stabilized Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
Mitsubishi Iupilon® H3000R 30 MFI Polycarbonate With Release Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 260 - 275 °C | 500 - 527 °F | |
Lavergne VYTEEN PC/ABS 3016 PC-ABS, 16% Glass Reinforced Vyteen PC/ABS 3016 is a black 16% glass fiber reinforced Polycarbonate/ABS alloy designed for injection molding.Features: -Good processability -Balanced stiffness/resilience -High deflection temp.. |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | |
Lavergne VYTEEN PC/ABS 8515XF Polycarbonate - Acrylonitrile Butadiene Styrene Alloy Vyteen PC/ABS 8515XF is an enhanced PC/ABS alloy with balanced impact/stiffness properties designed for injection molding applications.Features: -High resilience -Excellent processability -High d.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Start Point: 265°C |
Kingfa PA6-M25G20 20% Glass & 25% Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Front Barrel Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
LG Chemical LUPOY GN5151RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 238 Black 21 N PA66, DRY Description: Unreinforced and modified polyamide 66, with improved impact resistance, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYL A 238 offers excellent .. |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® A 60 G2 V30 PA66, 30% glass fiber, DRY Description: High flow Polyamide PA66 Flame retarded grade reinforced with 30% glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Applicat.. |
|||
Front Barrel Temperature | 260 - 270 °C | 500 - 518 °F | |
Solvay TECHNYL® B 230 PA66/6, DRY Description: Unreinforced and modified copolyamide 66/6, with high flexibility and improved impact resistance, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHN.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA), 50% Glass Fiber Ixef® 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Features: Good Ch.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 2030 Polyarylamide (PARA), 55% GlassMineral Ixef® 2030 is a 55% glass-fiber/mineral reinforced polyarylamide compound which exhibits high strength, very high stiffness, low warpage, excellent creep resistance and outstanding surface gloss... |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 30% Glass Fiber Reinforced Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 30% Glass Filled Impact Modified, Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 280 °C | 500 - 536 °F | Pre-3. Region Temperature |
Tisan TISLAMID® 66 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Front Barrel Temperature | 260 - 271 °C | 500 - 520 °F | |
Wellman Wellamid® GS40-60 42LH-N 40% Glass Sphere Filled Nylon 6, Lubricated & Heat Stabilized Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® 1027 Polyarylamide (PARA)
(Unverified Data**) Ixef 1027 is a 50% glass-fiber reinforced, heat stabilized polyarylamide, which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 102.. |
|||
Front Barrel Temperature | 260 - 290 °C | 500 - 554 °F | Nozzle Zone |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM
(discontinued **)< The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |