Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 257 - 282 °C | 495 - 540 °F | |
Star Plastics PC/PBT7820 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 257 - 282 °C | 495 - 540 °F | |
Star Plastics PC/PBTQX7008 Molding Grade PC/PBT Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 257 - 282 °C | 495 - 540 °F | |
Star Plastics PC/PET7901 Molding Grade PC/PET Information provided by Star Plastics, Inc. |
|||
Front Barrel Temperature | 257 - 274 °C | 495 - 525 °F | |
Teknor Apex Chemlon® 340G Nylon 610, Glass Fiber Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Front Barrel Temperature | 257 - 274 °C | 495 - 525 °F | |
Teknor Apex Chemlon® 345G Nylon 610, Glass Fiber Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |