Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 235 °C | 455 °F | For film or coating with EVA or EVOH. |
DuPont Bynel® 21E553 Adhesive Resin
(discontinued **) Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in.. |
|||
Front Barrel Temperature | 235 °C | 455 °F | |
DuPont Bynel® 30E699 Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Front Barrel Temperature | 235 °C | 455 °F | |
DuPont Bynel® 39E622 Adhesive Resin
(discontinued **) Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Front Barrel Temperature | 235 - 275 °C | 455 - 527 °F | Start Point: 255°C |
Kingfa JH830 Flame Retardant PC Features:UL V-0 @ 1.6mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInformation Prov.. |
|||
Front Barrel Temperature | 235 - 265 °C | 455 - 509 °F | Start Point: 235°C |
Kingfa JH960 6111 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesHigh heat resistanceChemical resistance, hydrolysis resistanceGood paint adhesionHigh flow ability,.. |
|||
Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
LG Chemical Lupox® GP1000M PBT Description: Injection Molding, PBT, High Flow, High ImpactApplication: Automotive (Connector)CAS No. 155123-66-3 and 24968-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
LG Chemical Lupox® GP1000SB PBT Description: Injection Molding, PBT, Anti-HydrolysisApplication: IT/OA, Automotive (Connector)CAS No. 24968-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | Injection Molding |
LG Chemical Lupox® GP1006FD PBT Description: Injection Molding, PBT, Flame Retardant, High ImpactApplication: IT/OA, Automotive (Connector)CAS No. 68928-70-1, 155123-66-3, 24968-12-5 and 1309-64-4Information provided by LG Chemica.. |
|||
Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
LG Chemical Lupox® GP-2000 General Purpose PBT, Unreinforced, Medium Viscosity LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
LG Chemical Lupox® SV-1120 General Purpose PBT, Unreinforced, High Molecular Weight, Extrusion LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Front Barrel Temperature | 235 - 255 °C | 455 - 491 °F | Injection Molding |
LG Chemical LUPOY GP5008A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, High FlowApplication: Miscellaneous GoodsCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
LG Chemical LUPOY HI5002A PC/ABS, High Impact Description: Injection Molding, PC/ABS, General Purpose, High Flow, High ImpactApplication: E&E (housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 235 - 265 °C | 455 - 509 °F | Injection Molding |
LG Chemical LUPOY MP5000AM PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Metal PlatingApplication: Automotive (Exterior), E&E (Housing)CAS: 103598-77-2 and 9003-56-9Information provided by LG Chemical |
|||
Front Barrel Temperature | 235 - 275 °C | 455 - 527 °F | Injection Molding |
LG Chemical LUPOY SG5009F PC/ABS Description: Injection Molding, PC/ABS, High Gloss, Scratch Resistance, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC & Monitor housing)CAS: 103598-77-2 and 181028-79-5Information prov.. |
|||
Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
LG Chemical Lupox® GP-1001F General Purpose PBT, Unreinforced, Flame Retardant LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
Solvay TECHNYL® C 402 M PA6, DRY Description: Unreinforced polyamide PA6, high viscosity, containing monomer, for extrusion.Available in: Europe and North AmericaProduct Applications: It is suitable for applications requiring high .. |
|||
Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
Solvay TECHNYLSTARâ„¢ S 216 V30 PA6, 30% glass filled, DRY Description: TECHNYL STAR TM Polyamide, reinforced with 30% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific, Europe and North AmericaPr.. |
|||
Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
Solvay TECHNYLSTARâ„¢ S 216 V35 PA6, 35% glass filled, DRY Description: TECHNYLSTAR polyamide, reinforced with 35% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North AmericaProduct Applications.. |
|||
Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
Borealis Borcoat™ BB127E Polypropylene Adhesive Powder form for Steel Pipe Coating Borcoat BB127E is a chemically modified polypropylene copolymer designed to be used as the tie layer between the epoxy corrosion protection layer and the Top-coat polypropylene coating Borcoat BB108.. |
|||
Front Barrel Temperature | 235 °C | 455 °F | |
DuPont Bynel® 39E660 Adhesive Resin Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Front Barrel Temperature | 235 °C | 455 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 4157 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Front Barrel Temperature | 235 °C | 455 °F | |
DuPont Bynel® 30E670 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Front Barrel Temperature | 235 - 271 °C | 455 - 520 °F | |
Diamond Polymers ASA S310 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Impact and ModulusInformation provided by Diamond Polymers, Inc. |
|||
Front Barrel Temperature | 235 - 271 °C | 455 - 520 °F | |
Diamond Polymers ASA S510 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Front Barrel Temperature | 235 - 271 °C | 455 - 520 °F | |
Diamond Polymers ASA S610 Description: ASA Weatherable Polymer, Injection Molding Grade, High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Front Barrel Temperature | 235 - 271 °C | 455 - 520 °F | |
Diamond Polymers ASA S910 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
Beijing Chemical Industry KAIFA® HN301-G0 PA6 Resin High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
Beijing Chemical Industry KAIFA® HN301-M30 PA6 Resin Mineral filled, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Front Barrel Temperature | 235 - 245 °C | 455 - 473 °F | |
Beijing Chemical Industry KAIFA® MN-401 PA6 Resin Good toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Front Barrel Temperature | 235 - 260 °C | 455 - 500 °F | Start Point: 240°C |
Kingfa JE2-R2G30 Glass Fiber Reinforced ABS/PBT Alloy Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a.. |