Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
Multibase Multi-Pro® 4008 T Polypropylene Talc Filled, 40% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: ConnectorsElectrical/Electronic ApplicationsAppliancesInformation provided by Multibase |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F4900-611UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT4500-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Automotive componentsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT4802-690UV Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT4900-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products G10P100-01UV 10% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: BracketsIP structural componentsDome light housingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products G10UP100-01 10% Glass Fiber Reinforced Polypropylene, Black, UL94-HB Rated Applications: Consumer housingsConsumer goodsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC8P200-00EG 8% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural, Extrusion Grade Applications: Extruded sheetWeather strippingInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP514-197 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 848 Black Applications: Mirror housingsInterior trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP514-199 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 195A Medium Neutral Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP514-438 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 167 Ebony Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products M15P100-01A 15% Mica Reinforced Polypropylene, Black Applications: Fan shroudsAir ductsElectronicsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products M15P101-01A 15% Mica Reinforced Polypropylene, Black Applications: Air ducts - distributionFan shroudsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products T10P100-00 10% Talc Reinforced Polypropylene, Natural Applications: Consumer goodsIP structural componentsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 227 °C | 399 - 441 °F | |
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene.. |
|||
Front Barrel Temperature | 204 - 227 °C | 399 - 441 °F | |
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o.. |
|||
Front Barrel Temperature | 204 - 216 °C | 399 - 421 °F | |
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE) Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat .. |
|||
Front Barrel Temperature | 204 °C | 400 °F | |
ExxonMobil Santoprene® 243-40 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Front Barrel Temperature | 204 °C | 400 °F | |
ExxonMobil Santoprene® 243-50 Thermoplastic Elastomer
(discontinued **) A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Front Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP522-286 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, ZUCA Medium Graphite Applications: ConsolesClose out panelInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 254 °C | 399 - 489 °F | |
PolyOne Dynaflex™ G7702-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7702-9001-02 is a performance TPE designed for a wide variety of applications. - Excellent Dimensional Stability - Excellent Heat Stability - High Resilience - Low Compression Set - Over.. |
|||
Front Barrel Temperature | 204 °C | 400 °F | |
Multibase Multi-Flex® TEA 4001-65 TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Front Barrel Temperature | 204 - 221 °C | 399 - 430 °F | |
Zhejiang Double Fish YS-G030 30% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Front Barrel Temperature | 204 - 221 °C | 399 - 430 °F | |
Zhejiang Double Fish YS-G040 40% Long Fiber Glass Reinforced Polypropylene Features high strength, good surface quality, and easy processing. Typical applications include automobile (bumper back beam, arm rest core, instrument panel, mudflap), machinery, electronics, comm.. |
|||
Front Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC SunPro® SP 200 P3081 Polypropylene Copolymer SunPro® SP 200 P 3081 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: GM PP .. |
|||
Front Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO CTC PP 2019 Polypropylene Impact Copolymer X-PRO PP 2019 is a high impact, polypropylene copolymer. It has automotive and industrial general purpose applications.Data provided by Composite Technologies (CTC). |
|||
Front Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO CTC PP 2025 Polypropylene Impact Copolymer X-PRO PP 2025 is an impact, polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Front Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
CTC X-PRO CTC PP 3020 Polypropylene Copolymer X-PRO PP 3020 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Front Barrel Temperature | 204 °C | 400 °F | |
ExxonMobil Santoprene® 123-50 Thermoplastic Elastomer
(discontinued **) A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ran.. |