Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 190 °C | 374 °F | |
Multibase TPSiV™ 3040-55A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Front Barrel Temperature | 190 °C | 374 °F | |
Multibase TPSiV™ 3340-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Front Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
Panipol Oy DXH-PP Inherently Conductive Polymer Panipol DXH-PP composition is conductive masterbatch for melt processing mainly with polypropylene. It is based on conductive Polyaniline and resin. Main benefits of Panipol DXH-PP grade are contr.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical AF312C ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical GPPS 25SP(E) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Front Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical LUCEL HI-515 High Impact POM, Unreinforced LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Front Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical LUCEL N109-AS Antistatic POM, Unreinforced, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Front Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical LUCEL N115-LD Anti Mold Deposit POM, Unreinforced, Internally Lubricated, Standard Viscosity LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Front Barrel Temperature | 190 - 200 °C | 374 - 392 °F | |
LG Chemical LUCEL N127-AS Antistatic POM, Unreinforced, High Flow LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Front Barrel Temperature | 190 - 200 °C | 374 - 392 °F | Injection Molding |
LG Chemical LUCEL N127LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Front Barrel Temperature | 190 - 215 °C | 374 - 419 °F | |
LG Chemical Lucet® N109 Acetal Copolymer Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical 80HF SAN, High Transparency, Heat Resistance, Chemical Resistance Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Front Barrel Temperature | 190 °C | 374 °F | Metering zone |
Taiwan PU Corporation TPUI-E90 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
Borealis Borcoat™ HE3453 Natural High Density Polyethylene for Steel Pipe Coating Borcoat HE3453 is a natural and colorable high density polyethylene produced with the Borstar technology in similar conditions as the black ready made top coat Borcoat HE3450. Borcoat HE3453 is rec.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® 30% Glass Fiber Reinforced Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® 30% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® 40% Calcite Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISREN® Flame Retardant (V0) Polystyrene TISREN has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimensio.. |
|||
Front Barrel Temperature | 190 - 220 °C | 374 - 428 °F | |
Unitika TERRAMAC HV-6250H Polylactic Acid (PLA) Foam, Extrusion, blow, and foam sheet grades. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® 20% Talc Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 °C | 374 °F | Injection |
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Front Barrel Temperature | 190 °C | 374 °F | Injection |
Alliance Polymers Viprene™ P80A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P80A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Front Barrel Temperature | 190 °C | 374 °F | Injection |
Alliance Polymers Viprene™ P85A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Front Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Pre-3. Region Temperature |
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Front Barrel Temperature | 190 - 220 °C | 374 - 428 °F | Extrusion |
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec.. |