Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
Star Plastics PC/ABSFR9002 Molding Grade PC/ABSFR Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 260 - 274 °C | 500 - 525 °F | |
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 257 - 274 °C | 495 - 525 °F | |
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by.. |
|||
Middle Barrel Temperature | 257 - 274 °C | 495 - 525 °F | |
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: .. |
|||
Middle Barrel Temperature | 257 - 274 °C | 495 - 525 °F | |
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade Notes: Medium-Impact; General Purpose; Impact modified to provide excellent toughness Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS-DB41 CPN3992 Color: W.. |
|||
Middle Barrel Temperature | 263 - 274 °C | 505 - 525 °F | |
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St.. |
|||
Middle Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
CTC X-PRO PP 100 P1015 Polypropylene Homopolymer X-PRO PP 1015 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Middle Barrel Temperature | 263 - 274 °C | 505 - 525 °F | |
Teknor Apex Chemlon® 133 G Nylon 66, 33% Short Glass Fiber Filled Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex |
|||
Middle Barrel Temperature | 257 - 274 °C | 495 - 525 °F | |
Teknor Apex Chemlon® 140 MH Nylon 66, 40% Mineral Reinforced Notes: 40% Mineral; High rigidity with exceptional control of warpage and surface sink marks; Excellent for large parts; Fast cycling Features: Fast Molding Cycle; High Rigidity; Heat Stabilized; Lo.. |