Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 277 - 299 °C | 531 - 570 °F | |
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, .. |