Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 275 - 290 °C | 527 - 554 °F | Injection Molding |
LG Chemical LUMID LW4303B(W) PA66+MF30%, Low Warpage Feature: Injection Molding, PA66+MF30%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 275 - 290 °C | 527 - 554 °F | Injection Molding |
LG Chemical LUMID LW4403B(W) PA66+GF/MF40%, Low Warpage Feature: Injection Molding, PA66+GF/MF40%, Low WarpageApplication: Automotive PartsCAS No. 32131-17-2, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 275 - 290 °C | 527 - 554 °F | Injection Molding |
LG Chemical LUPOY GN1002FC PC, Halogen Free, Flame Retardant, High Impact Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 25232-40-0 and 139189-30-3Information .. |
|||
Middle Barrel Temperature | 275 - 290 °C | 527 - 554 °F | Injection Molding |
LG Chemical LUPOY GN1002FH PC, Halogen Free, Flame Retardant, Heat Resistant Description: Injection Molding, PC, Halogen Free Flame Retardant, Heat Resistant, Chemical Resistance, High ImpactApplication: IT/OA Housing and Components (Adaptor)CAS: 103598-77-2, 25232-40-0 and .. |
|||
Middle Barrel Temperature | 275 - 290 °C | 527 - 554 °F | Injection Molding |
LG Chemical LUPOY GN1002FL PC, Halogen Free, Flame Retardant, High Flow Description: Injection Molding, PC, Halogen Free Flame Retardant, High Flow, High ImpactApplication: IT/OA (M/P Battery Inner Pack Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information pro.. |
|||
Middle Barrel Temperature | 275 - 290 °C | 527 - 554 °F | Injection Molding |
LG Chemical LUPOY GN1002FS PC, Halogen Free, Flame Retardant, High Impact Description: Injection Molding, PC, Halogen Free Flame Retardant, High Impact, Chemical ResistanceApplication: IT/OA (M/P Battery Housing)CAS: 103598-77-2, 25232-40-0 and 139189-30-3Information prov.. |
|||
Middle Barrel Temperature | 275 - 280 °C | 527 - 536 °F | Compression Zone |
Solvay Technyl® A20V25 25% Glass Filled, V-0 Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Middle Barrel Temperature | 275 - 290 °C | 527 - 554 °F | |
Teknor Apex Beetle® PET1610F Polyethylene Terephthalate, 50% Glass Fiber Reinforced Notes: PET1610F is a 50% glass fiber reinforced grade of PET that offers good mechanical performance at elevated temperatures and excellent mold release. Processing Method: Injection Molding Forms: .. |
|||
Middle Barrel Temperature | 275 - 285 °C | 527 - 545 °F | Zone 2 |
Eurostar Starflam AFR450X1 PA66, 25% Glass Filled, Injection Molded AFR450X1 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Middle Barrel Temperature | 275 - 285 °C | 527 - 545 °F | Zone 2 |
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su.. |
|||
Middle Barrel Temperature | 275 - 285 °C | 527 - 545 °F | Zone 2 |
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
Middle Barrel Temperature | 275 - 285 °C | 527 - 545 °F | Zone 2 |
Eurostar Starflam RF0023E PA66/6, 10% Glass Filled, Injection Molded Starflam RF0023E is a Mineral Flame Retardant, Halogen Free and Phosphorous Free, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding (also known as RF1002Z230EM)Information provided by Polymer.. |