Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 250 - 265 °C | 482 - 509 °F | |
Parker Chomerics PREMIER™ A220-FR EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Middle Barrel Temperature | 250 °C | 482 °F | Zone 2; Cylinder |
Premix Thermoplastics PRE-ELEC® PPE 1461
(discontinued **) PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Middle Barrel Temperature | 250 °C | 482 °F | Zone 1; Cylinder |
Premix Thermoplastics PRE-ELEC® PPE 1461
(discontinued **) PRE-ELEC PPE 1461 is a conductive thermoplastic compound based on modified polyphenylene ether (PPE). Conductivity is achieved by using special conductive carbon black. In addition to a low electric.. |
|||
Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Homogenization Zone |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, DAM
(discontinued **) The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Homogenization Zone |
Solvay Specialty Polymers Ixef® 3006/9019 Polyarylamide, 30% Carbon Fiber, at Equilibrium (65% RH)
(discontin The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Middle Barrel Temperature | 250 - 290 °C | 482 - 554 °F | Start Point: 275°C |
Kingfa JH720 G50 50% Glass Fiber Reinforced PC Features:Excellent balance propertiesSuper high stiffnessHigh hardnessGood size stabilitySuper high mechanical strengthApplications:Imaging equipment shellOA body frameElectrical equipmentComputer p.. |
|||
Middle Barrel Temperature | 250 - 270 °C | 482 - 518 °F | |
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 250 - 270 °C | 482 - 518 °F | |
LG Chemical Lupox® PBT-HI1002FM Impact Modified, Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® SG3250M PBT+PET+MF25% Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® SG5200 PBT+PET+GF20% Description: Injection Molding, PBT+PET+GF20%, Good Surface Application: E&E (Microwave Oven Door Gasket)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Injection Molding |
LG Chemical LUPOY HP5004A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2, 9003-56-9 and 18102.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Lavergne VYPET VNT 1020 Polyester-PC Alloy The Vypet 1020 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Lavergne VYPET VNT 1021 Polyester-PC Alloy The Vypet 1021 Black is a medium viscosity Polyester and PC alloy, has an excellent balance of stiffness and impact resistance.Features: Excellent Processability; Good Impact Resistance; Good Chemic.. |
|||
Middle Barrel Temperature | 250 - 270 °C | 482 - 518 °F | Start Point: 255°C |
Kingfa PA6-M20G16 20% Glass & 16% Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Injection Molding |
LG Chemical Lupox® SG5500 PBT+PET+GF50% Description: Injection Molding, PBT+PET+GF50%, Good Surface, High StiffnessApplication: E&E, Automotive (Switch)CAS No. 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Middle Barrel Temperature | 250 - 290 °C | 482 - 554 °F | Injection Molding |
LG Chemical LUPOY GN5007FL PC/ABS, Halogen Free Flame Retardant, Heat Resistance Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, Heat Resistance, High FlowApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 9003-56-9 and 181028.. |
|||
Middle Barrel Temperature | 250 - 255 °C | 482 - 491 °F | Compression Zone |
Solvay Technyl® C 218 MT25 V15 25% Mineral, 15% Glass Filled, Heat Stabilized Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | |
Teknor Apex Beetle® PBTC115F Polybutylene Terephthalate and Polyethylene Terephthalate Notes: PBTC115F is a 15% glass fiber reinforced PBT/PET alloy. It provides a good balance of mechanical performance and thermal endurance with excellent surface finish and mold release. Features: G.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | |
Unitika A1030GFL PA6, 30% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 250 °C | 482 °F | |
Tipco Tipcofil® AG 300 - 15% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 15% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 2 |
Eurostar Starflam PZ0042E PA6, 20% Glass Filled, Injection Molded PZ0042E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1004Z222 or PA620GFU9Z22)Information provided by Polymer Technol.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 2 |
Eurostar Starflam PF0057E PA6, 25% Glass Filled, Injection Molded Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF-1005 Z270)Information provided by Polymer Technology & Services,.. |
|||
Middle Barrel Temperature | 250 - 260 °C | 482 - 500 °F | Zone 2 |
Eurostar Starflam PK0052E PA6, 25% Mineral Filled, Injection Molded PK0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Mineral Filed, Polyamide 6 Injection Molding (also known as PM3520Z222 or PA 25E6 U9 Z22)Information provided by Polymer Technolo.. |
|||
Middle Barrel Temperature | 250 - 300 °C | 482 - 572 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) 60G5F Nylon 66, 25% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Middle Barrel Temperature | 250 - 300 °C | 482 - 572 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) 6010FGN Nylon 66 Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Middle Barrel Temperature | 250 - 300 °C | 482 - 572 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) 60G7F Nylon 66, 35% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Middle Barrel Temperature | 250 - 300 °C | 482 - 572 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) 60T6 Nylon 66, 30% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Homogenization Zone |
Solvay Specialty Polymers Ixef® 1501/0003 Polyarylamide, 30% Glass Fiber, at Equilibrium (65% RH)
(discontinu The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Middle Barrel Temperature | 250 - 280 °C | 482 - 536 °F | Homogenization Zone |
Solvay Specialty Polymers Ixef® 2530/X9027 Polyarylamide, 55% Mineral + Glass Fiber, DAM
(discontinued **)< The IXEF compounds are a family of semi-crystalline polyarylamide thermoplastics reinforced with glass fibers and/or mineral fillers for injection molding.Data provided by the manufacturer, Solvay A.. |
|||
Middle Barrel Temperature | 250 - 300 °C | 482 - 572 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) ST60G3 Nylon 66, 15% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |