Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 230 °C | 446 °F | |
NYCOA 1838 Copolymer Nylon Alloy good impact resistant molding and extrusion gradeInformation provided by NYCOA, Inc. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | |
NYCOA 2263 Copolymer Nylon Alloy monofilament weed eater, fishing lineInformation provided by NYCOA, Inc. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | |
NYCOA 27/300I Glass Filled Nylon 6 30% glass filled, flame retardant to UL 94 V-0 nylon 6Information provided by NYCOA, Inc. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | |
NYCOA 27/300SR Glass Filled Nylon 6 30% glass filled, flame retardant to UL 94 H-B nylon 6Information provided by NYCOA, Inc. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | |
NYCOA 27/330KNF Glass Filled Nylon 6 33% glass filled, heat stabilized nylon 6Information provided by NYCOA, Inc. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | |
NYCOA 7551 Copolymer Nylon Alloy resistant to zinc chloride and other automotive fluids, good adhesion to olefins, mold & extrusion.Information provided by NYCOA, Inc. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | Zone 5; Cylinder |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | Zone 6; Cylinder |
Premix Thermoplastics PRE-ELEC® PS 1324 PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Middle Barrel Temperature | 230 °C | 446 °F | Zone 5; Cylinder |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Gichem GIBLEND F70X3/VO ABS - Polycarbonate - PC/ABS Flame Retardant
(discontinued **) Blend PC-ABS self-extinguishing class V0 high fluidity. Medium injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegis™ H135XP Nylon 6 Extrusion Grade Homopolymer Film
(discontinued **) Description: Aegis H135XP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegisâ„¢ H100QP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H100QP is a lubricated medium viscosity, Nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500 as well as EU Directiv.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | Cast Film |
Honeywell Aegisâ„¢ H135ZP Nylon 6 Extrusion Grade Homopolymer Film Description: Aegis H135ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 for nylon.. |
|||
Middle Barrel Temperature | 230 - 255 °C | 446 - 491 °F | Start Point: 225°C |
Kingfa JH960 6300 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platin.. |
|||
Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 240°C |
Kingfa PBT-T30 30% Mineral Filled PBT Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
LG Chemical LUMAX GP-5106F General Purpose PBT, 10% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | Injection Molding |
LG Chemical LUMAX GP5200B PBT+ABS+GF20% Description: Injection Molding Grade, PBT+ABS+GF20%, General PurposeApplication: E&E (Speaker Frame)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 9003-54-7Information provided by LG Chemical |
|||
Middle Barrel Temperature | 230 - 245 °C | 446 - 473 °F | |
LG Chemical LUMAX HR-5306F Heat Resistant PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
LG Chemical Lupox® GP-1006F General Purpose PBT, Unreinforced, Flame Retardant, Non-Bleed LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
LG Chemical Lupox® GP-2000 General Purpose PBT, Unreinforced, Medium Viscosity LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Middle Barrel Temperature | 230 - 270 °C | 446 - 518 °F | |
LG Chemical LUPOY HR-5007AX Heat Resistant PC/ABS Alloy, Unreinforced Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Middle Barrel Temperature | 230 - 260 °C | 446 - 500 °F | |
Gromax 1172LL TPE 1172LL is high modulus grade with nominal Durometer hardness of 72D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like blow molding grade. Charac.. |
|||
Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
LG Chemical Lupox® GP-1001F General Purpose PBT, Unreinforced, Flame Retardant LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH0 Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal .. |
|||
Middle Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Compression Zone |
Solvay Technyl® C218V30 30% Glass Filled, Heat Stabilized Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Middle Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samyang Tribit® 1500G30 Polybutylene Terephthalate, 30% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Middle Barrel Temperature | 230 - 265 °C | 446 - 509 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) 30G6 Polybutylene terephthalate, 30% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Middle Barrel Temperature | 230 - 265 °C | 446 - 509 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) 30G6F Polybutylene terephthalate, 30% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |