Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
Multibase Multi-Pro® 2006 T Polypropylene Talc Filler, 20% by weight.Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products F52-01 20% Mica Reinforced Polypropylene Copolymer, Black Applications: Functional support ductsHousingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products FT4650-581UV Thermoplastic Polyolefin, UV Stabilized, HD2 Medium Quartz Metallic Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products G20P100-01UV 20% Glass Fiber Reinforced Polypropylene, UV Stabilized, Black Applications: Rigid exterior componentsHousingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC20P100-177UV 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, (Chrysler HS5) Gray Applications: Air Ducts - distributionBracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP517-00 23% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trim moldingsSill platesTire coverInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products HP800-706UV 20% Talc Reinforced High Performance Polypropylene Copolymer, Scratch Resistant, UV Stabilized, Impact Modified, SWB White Applications: Interior trim/Instrument panel componentsA/B pillarsGlove box doorsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products M20P100-01 20% Mica Reinforced Polypropylene, Black Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products RCT220-01 20% Talc Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: Fan shroudsElectrical housingsHush panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products T20P100-01 20% Talc Reinforced Polypropylene, Black Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products T20P250-699UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AC20157-120 Black Applications: Window trimCowl screensExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LCF50 - PP Homopolymer Polypropylene, 50% Long Carbon Fiber Reinforced Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc. |
|||
Middle Barrel Temperature | 204 - 216 °C | 400 - 420 °F | |
PlastiComp Complet® LGF50 - PP Homopolymer Polypropylene, 50% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polypropylene with 50% long glass fiber reinforcementInformation provided by PlastiCom.. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/10 Polypropylene Homopolymer, 10% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/20/FR Polypropylene Homopolymer, 20% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/30/E/NS Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, NSF listed Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/20/E/HF Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-60/20/E8/M Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
Star Plastics ABS405 Extrusion Grade ABS Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
Star Plastics ABSGF10 Molding Grade ABS With 10% Glass Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
Star Plastics ABS3545 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Middle Barrel Temperature | 204 °C | 400 °F | |
Chi Mei Polylac® PA-765 ABS - Flame Retardant F.R. High Flow |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products CC20P200-01 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Black Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
LTL Color Compounds ColorFast® GPA100 ABS High impact, high gloss injection molding ABS, HB-rated, FDAAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
LTL Color Compounds ColorFast® GPA300 ABS Super-tough ABS with our highest impact strength, injection moldingAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
LTL Color Compounds ColorFast® GPA300X ABS Extrusion grade, high impact, high gloss ABSAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-68/30/E/UV Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
RheTech Products GC20P255-712UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, B231 Earth Grey Applications: Consumer goodsMiscellaneous bracketsExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |