Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 177 - 199 °C | 351 - 390 °F | |
PolyOne Versaflex™ CL30 Thermoplastic Elastomer (TPE) Versaflex™ CL30 is an easy processing compound designed for use in injection molding and extrusion applications where water-clarity and excellent colorability are required. - Excellent Clarity - Ex.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE) Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 351 - 390 °F | |
PolyOne Versaflex™ OM 2262 Thermoplastic Elastomer (TPE) Versaflex™ OM 2262 is a performance overmolding grade with general FDA compliance. This product is designed for both insert and two-shot molding onto Eastman Tritan™ copolyester as well as ABS, PC.. |
|||
Middle Barrel Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Dynaflex™ G6713-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G6713-0001 is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV.. |
|||
Middle Barrel Temperature | 177 - 216 °C | 351 - 421 °F | |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 351 - 390 °F | |
PolyOne Dynaflex™ G7650-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynaflex™ G7670-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynaflex™ G7670-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7670-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Middle Barrel Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Dynaflex™ G7680-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7680-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynaflex™ G7690-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7690-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynaflex™ G7940-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynaflex™ G7940-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7940-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhesion.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 351 - 390 °F | |
PolyOne Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1001-00 is an easy processing, general purpose material designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypro.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Middle Barrel Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Dynaflex™ G7960-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Middle Barrel Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Dynaflex™ G7970-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Middle Barrel Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Dynaflex™ G7980-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7980-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Middle Barrel Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Dynaflex™ G7990-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7990-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-1001-00 can be re.. |
|||
Middle Barrel Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Dynaflex™ G7990-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7990-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-9001-02 can be re.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynalloy™ OBC 8100-N75 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N75 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Middle Barrel Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Dynaflex™ G2709-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2709-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone/UV Stability - Overmol.. |
|||
Middle Barrel Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Dynaflex™ G6713C Thermoplastic Elastomer (TPE) Dynaflex™ G6713C is an easy processing TPE designed for use in injection molding and extrusion applications where an extremely soft feel is desired. - Excellent Colorability - Good Ozone and UV Sta.. |
|||
Middle Barrel Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Dynaflex™ G7650-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7650-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynaflex™ G7660-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7660-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop.. |
|||
Middle Barrel Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Dynaflex™ G7960-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7960-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynaflex™ G7970-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Middle Barrel Temperature | 177 - 188 °C | 351 - 370 °F | |
PolyOne Dynaflex™ G7980-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7980-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Middle Barrel Temperature | 177 - 193 °C | 351 - 379 °F | |
PolyOne Dynalloy™ OBC 8100-N65 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N65 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Middle Barrel Temperature | 177 - 199 °C | 351 - 390 °F | |
PolyOne Dynalloy™ OBC8000-T60 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8000-T60 is an easy processing, general processing TPE utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. Designed for a wide variety of applications, incl.. |