Processing Properties Metric English Comments
Middle Barrel Temperature 246 - 274 °C
475 - 525 °F
PTS PCA-2010NH Non-Bromine, Non-Chlorine, Flame Retardant PC/ABS Alloy
This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 246 - 274 °C
475 - 525 °F
PTS PCA-FR Eco-Friendly, High Flow, Flame Retardant PC/ABS Alloy
This is a non-halogenated flame retardant grade. Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 246 - 274 °C
475 - 525 °F
PTS PCA-2010NHV Non-Bromine, Non-Chlorine, Flame Retardant UV PC/ABS Alloy
This is a non-halogenated flame retardant, UV stabilized grade. Information provided by Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 246 - 274 °C
475 - 525 °F
Star Plastics PC/ABSFR9001 Molding Grade PC/ABSFR
Information provided by Star Plastics, Inc.
Middle Barrel Temperature 246 - 274 °C
475 - 525 °F
Star Plastics PC/ABSFR9002 Molding Grade PC/ABSFR
Information provided by Star Plastics, Inc.
Middle Barrel Temperature 260 - 274 °C
500 - 525 °F
Star Plastics PC/ABSQX7005 Molding Grade PC/ABS
Information provided by Star Plastics, Inc.
Middle Barrel Temperature 257 - 274 °C
495 - 525 °F
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced
Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by..
Middle Barrel Temperature 257 - 274 °C
495 - 525 °F
Teknor Apex Chemlon® 100 Nylon 66, Unreinforced
Features: Basic nylon 66 with internal lubrication. Widely used for automotive, electronic and appliance applications. Processing Method: Injection Molding Forms: Pellets Automotive Specifications: ..
Middle Barrel Temperature 257 - 274 °C
495 - 525 °F
Teknor Apex Chemlon® 104 Nylon 66, Impact Grade
Notes: Medium-Impact; General Purpose; Impact modified to provide excellent toughness Processing Method: Injection Molding Forms: Pellets Automotive Specifications: Chrysler MS-DB41 CPN3992 Color: W..
Middle Barrel Temperature 263 - 274 °C
505 - 525 °F
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced
Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St..
Middle Barrel Temperature 246 - 274 °C
475 - 525 °F
CTC X-PRO PP 100 P1015 Polypropylene Homopolymer
X-PRO PP 1015 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled..
Middle Barrel Temperature 263 - 274 °C
505 - 525 °F
Teknor Apex Chemlon® 133 G Nylon 66, 33% Short Glass Fiber Filled
Notes: Flammability: Passes, FMVSS 302 Processing Method: Injection Molding Forms: Pellets FMVSSInformation Provided by Teknor Apex
Middle Barrel Temperature 257 - 274 °C
495 - 525 °F
Teknor Apex Chemlon® 140 MH Nylon 66, 40% Mineral Reinforced
Notes: 40% Mineral; High rigidity with exceptional control of warpage and surface sink marks; Excellent for large parts; Fast cycling Features: Fast Molding Cycle; High Rigidity; Heat Stabilized; Lo..