Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 220 - 230 °C | 428 - 446 °F | |
Gichem GILAC F80X5/V0 ABS Flame Retardant
(discontinued **) ABS self-extinguishing class V0. Medium injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
Kingfa FRHIPS-980 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance properties, Non-DPOExcellent heat stability & electrical propertyColor tailor-made for clientApplications:Injection moldingGas assistant mold.. |
|||
Middle Barrel Temperature | 205 - 230 °C | 401 - 446 °F | Start Point: 215°C |
Kingfa HIPS-5197 High Impact Polystyrene Features:UL 94 HB @ 1.6mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientsApplications:Injection moldingGas assistant moldingTV & Audio housingElec.. |
|||
Middle Barrel Temperature | 180 - 230 °C | 356 - 446 °F | Injection |
Kolon DIAMAT® GP Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Middle Barrel Temperature | 180 - 230 °C | 356 - 446 °F | Injection |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL ED1045D TPO, Thermoplastic Elastomer Description: Injection Molding, TPO, Thermoplastic Elastomer, Soft TouchApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 1333-86-4, 25087-34-7 and 14807-96-6Information provided.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL EI5002L PP Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 9002-88-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3202B PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HF5254A PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | |
LG Chemical LUPOL HG-3200 High Gloss Polypropylene, 20% Mineral Fillers LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HI5204H PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL TE5107 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL TE5108H PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL TE5109 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL TE5208 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Middle Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical XR401B ABS, High Flow, Heat Resistance Feature: Injection Molding, High Flow, Heat ResistanceApplication: Automotives Exterior Housing (Side Mirror Housing, Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information p.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3402 PP+MF40% Description: Injection Molding, PP+MF40%, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HM3102A PP+MF10%, High Impact Description: Injection Molding, PP+MF10%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsInformation provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL HM3207SM PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, Good Weatherability, High ImpactApplication: Automotive Interior Parts CAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL LW4405 PP+GF/MF40% Description: Injection Molding, PP+GF/MF40%, Low WarpageApplication: Electrical, Electronic and Automotive Parts CAS: 9003-07-0, 65997-17-3 and 12001-26-2Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | |
LG Chemical LUPOL TE-5005H Thermoplastic Elastomer Alloy, Dimensional Stability LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL TE5007B PP+Rubber, High Impact Description: Injection Molding, PP+Rubber, Low Density, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia , Rear Bumper Step)Information provided by LG Chemical |
|||
Middle Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
LG Chemical XR401T ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Electric & Electronic Housing (Frame etc) Automotives Interior & Exterior Housing (Garnish etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9.. |
|||
Middle Barrel Temperature | 190 - 230 °C | 374 - 446 °F | |
Borealis BB412E Polypropylene Block Copolymer for extrusion and injection BB412E is a natural, medium molecular weight, medium melt flow rate polypropylene block copolymer with an optimal mechanical properties balance resulting in high stiffness and very good impact stren.. |
|||
Middle Barrel Temperature | 190 - 230 °C | 374 - 446 °F | |
Borealis HA104E Polypropylene Homopolymer HA104E is a natural high molecular weight, high melt flow rate polypropylene homopolymer characterized by well-balanced stiffness to impact strength ratio at increased processing properties. Applica.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Pipe Extrusion |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Middle Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3100 PP+MF10% Description: Injection Molding, PP+MF30%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 200 - 230 °C | 392 - 446 °F | Injection Molding |
LG Chemical LUPOL GP3102 PP+MF10%, High Impact Description: Injection Molding, PP+MF10%, General Purpose, High ImpactApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |