Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 96.0 °C | 205 °F | barrel 1 |
Borealis FR4830 Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires FR4830 is a chemically crosslinkable Non-halogen flame retardant Polyethylene compound for Primary Automotive and Appliance Wire. Applications: FR4830 is intended for use as a 125º C rated primary .. |
|||
Middle Barrel Temperature | 96.0 °C | 205 °F | barrel 1 |
Borealis FR4837 Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires FR4837 is a chemically crosslinkable Non-halogen flame retardant Polyethylene compound for Primary Automotive and Appliance Wire. Applications: FR4837 is intended for use as a 125º C rated primary.. |
|||
Middle Barrel Temperature | 96.0 °C | 205 °F | barrel 1 |
Borealis FR4832 Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires FR4832 is a Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires. Applications: FR4832 is intended for use as a 125º C rated primary insulation for crosslinked automotive wi.. |