Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 282 - 293 °C | 540 - 560 °F | |
Polymer Resources NY6/12-G33 Nylon 612, 33% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 282 - 293 °C | 540 - 560 °F | |
Polymer Resources NY6/12-G43 Nylon 612, 43% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Middle Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Polymer Resources NY66-FRG25 Flame Retardant Nylon 66, 25% Glass Reinforced Nylon 66, 25% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are.. |
|||
Middle Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Polymer Resources NY66-IM1-G13 Nylon 66, 13% Glass Reinforced, Toughened Nylon 66, 13% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Middle Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Polymer Resources NY66-IM1-G33-[color]-H Nylon 66, 33% Glass Reinforced, Toughened and Heat Stabilized Nylon 66, 33% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Middle Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Polymer Resources NY66-IM-G40 Nylon 66, 40% Glass Reinforced, Impact Modified Nylon 66, 40% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Middle Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Polymer Resources NY66-M25G15 Nylon 66, 25% Mineral, 15% Glass Reinforced Nylon 66, 25% Mineral, 15% Glass Reinforced, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon gr.. |
|||
Middle Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Polymer Resources NY66-M25G15-[color]-H Nylon 66, 25% Mineral, 15% Glass Reinforced, Heat Stabilized Nylon 66, 25% Mineral, 15% Glass Reinforced, Lubricated and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, te.. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-FD2-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-FR2A-D-[color]-3 Polycarbonate, Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-FR2-D-[color]-3 Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-FR2-TFE Polycarbonate, Flame Retardant, 5% PTFE Polycarbonate, Improved Flame Retardant, 5% PTFE LubricantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-GP2-D Polycarbonate, General Purpose, Medium Flow Polycarbonate, General Purpose, Medium FlowFeatures: • Ultra High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on.. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-GP2-D-[color]-1 Polycarbonate, General Purpose, Medium Flow with Mold Release Polycarbonate, General Purpose, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf.. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-GP2-D-[color]-5 Polycarbonate, FDA-compliant Feedstocks, Medium Flow Polycarbonate, FDA-compliant Feedstocks, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-GP2-D-[color]-6 Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold Release Polycarbonate, FDA-compliant Feedstocks, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-IM1 Polycarbonate, Impact Modified, Low Flow Polycarbonate, Impact Modified, Low FlowProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized Polycarbonate, Impact Modified, Low Flow, UV-stabilizedProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Middle Barrel Temperature | 282 - 299 °C | 540 - 570 °F | |
Polymer Resources NY66-IM1-G13-[color]-H Nylon 66, 13% Glass Reinforced, Toughened and Heat Stabilized Nylon 66, 13% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-FD2 Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Medium Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sam.. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
Polymer Resources PC-UV2-D Polycarbonate, UV-stabilized, Medium Flow Polycarbonate, UV-stabilized, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Middle Barrel Temperature | 282 - 293 °C | 540 - 560 °F | |
PTS Tristar® PC-10FR-(8) 8 MFI Flame Retardant Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 282 - 293 °C | 540 - 560 °F | |
PTS Tristar® PC-10FR-(V8) 8 MFI Flame Retardant, UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 282 - 293 °C | 540 - 560 °F | |
PTS Tristar® PC-10R-(8) 8 MFI Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 282 - 293 °C | 540 - 560 °F | |
PTS Tristar® PC-10R-(V8) 8 MFI UV Stabilized Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
LTL Color Compounds ColorFast® PC100 Polycarbonate 10 melt standard injection molding gradeAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 282 - 293 °C | 540 - 560 °F | |
Wellman Wellamid® MRGF25/15 22H-N 25% Mineral/15% Glass Fiber Reinforced Nylon 66, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Middle Barrel Temperature | 282 °C | 540 °F | |
Teknor Apex Chemlon® 109-33 GH Nylon 66, 33% Glass Fiber Filled Notes: High-Impact; Reinforced with 33% Glass Fibers; Highly toughened compound exhibiting strength and rigidity Features: Good Creep Resistance; Good Stiffness; High Strength; Good Impact Resistanc.. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
LTL Color Compounds ColorFast® FRPC100 Polycarbonate, Flame-Retarded Flame-retarded V0, high impact injection molding polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 282 - 304 °C | 540 - 580 °F | |
LTL Color Compounds ColorFast® FRPC200 Polycarbonate, Flame-Retarded Improved flame-retarded V0/5V injection molding polycarbonateAll information provided by LTL Color Compounders, Inc. |