Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 270 °C | 518 °F | Zone 6; Cylinder |
Premix Thermoplastics PRE-ELEC® PC 1431 PRE-ELEC PC 1431 is a conductive thermoplastic compound based on polycarbonate. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Middle Barrel Temperature | 270 - 320 °C | 518 - 608 °F | Injection Molding |
LG Chemical LUCON SP9306FL sPS+MF Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 .. |
|||
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F | Injection Molding |
LG Chemical LUMID EG2309B(W) PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol) Feature: Injection Molding, PA66+GF30%, Chemical Resistance(CaCl2, Ethylene Glycol)Application: Radiator Tank, Intercooler TankCAS No. 32131-17-2, 65997-17-3 and 9010-79-9Information provided by LG .. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID GP2151BF PA66+GF15%, Flame Retardant Feature: Injection Molding, PA66+GF15%, Halogen Free Flame RetardantApplication: ConnectorsCAS No. 32131-17-2, 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG.. |
|||
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F | Injection Molding |
LG Chemical LUMID GP2500B(W) PA66+GF50%, General Purpose Feature: Injection Molding, PA66+GF50%, General PurposeApplication: Automotive (Gear Shift Housing)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Injection Molding |
LG Chemical LUMID GP3200B(W) PA66+MF20%, General Purpose Feature: Injection Molding, PA6+MF20%, General PurposeApplication: E&E (Rice Cooker Housing)Information provided by LG Chemical |
|||
Middle Barrel Temperature | 270 - 275 °C | 518 - 527 °F | |
Lavergne VYPET VNT 230 PET - PBT 30% Glass Reinforced Polyester Vypet VNT 230 is a 30% fiberglass reinforced modified PBT/PET polyester injection molding compound designed for electrical applications requiring improved surface aesthetics and improved UV resistan.. |
|||
Middle Barrel Temperature | 270 - 290 °C | 518 - 554 °F | |
Teknor Apex Beetle® 66GS6 Nylon 66, 30% Glass Bead Reinforced Notes: 66GS6 is a 30% glass sphere filled nylon 66 that offers increased rigidity coupled with low distortion Features: High Rigidity; Low Warpage Processing Method: Injection Molding Forms: Pellet.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Compression Zone |
Solvay Technyl® A 216 V40 40% Glass Filled Nylon 66 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Middle Barrel Temperature | 270 - 290 °C | 518 - 554 °F | |
Teknor Apex Chemlon® ALF20 Nylon 66, Unreinforced Notes: ALF20 is a self-lubricating grade of nylon 66 containing PTFE and Silicone. It offers outstanding surface wear characteristics of molded parts. It is suitable for applications such as beari.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH0 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | |
Solvay Technyl® A 216 V30 Nylon 66, 30% Glass Fiber, EH50 Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Technyl A 216 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical prope.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Mid-2. Region Temperature |
Tisan TISARBON® Flame Retardant (V0) Polycarbonate TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Zone 2 |
Eurostar Staramide AG10 PA66, 50% Glass Filled, Injection Molded AG10 is a 50% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Zone 2 |
Eurostar Staramide AG4 PA66, 20% Glass Filled, Injection Molded AG4 is a 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F | Zone 2 |
Eurostar Staramide RFB24 PA66, 20/10% Glass Fiber/Glass Bead Filled Injection Molded RFB24 is a Glass Bead and Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as Staramide 66 2010VK Z3)Information provided by Polymer Technology & Services, the North American.. |
|||
Middle Barrel Temperature | 270 - 280 °C | 518 - 536 °F | Zone 2 |
Eurostar Staramide AG3 PA66, 15% Glass Filled, Injection Molded AG3 is a 15% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F | |
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, DAM Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good.. |
|||
Middle Barrel Temperature | 270 - 310 °C | 518 - 590 °F | |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Middle Barrel Temperature | 270 - 285 °C | 518 - 545 °F | |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |
|||
Middle Barrel Temperature | 270 - 320 °C | 518 - 608 °F | |
LG Chemical LUCON CP-4208F Conductive Thermoplastic, Flame Retardant LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |