Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 240 °C | 464 °F | |
Multibase TPSiV™ 1180-50D Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Middle Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Start Point: 250°C |
Kingfa JH710 G10D Flame Retardant & 10% Glass Fiber Reinforced PC Features:Environmental friendly flame retardantUL V-0 @ 1.6mmHigh mechanical strengthGood size stability, good surfaceSuitable for exact moldingApplications:Exact mechanism partsElectrical and elect.. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Start Point: 235°C |
Kingfa MAC-601 UV PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou.. |
|||
Middle Barrel Temperature | 240 - 255 °C | 464 - 491 °F | Start Point: 245°C |
Kingfa PA66-ROW Halogen-free, Flame Retardant PA66 Features:Flame retardantHigh mechanical strengthHigh heat resistanceGood electric propertiesNo bloomingApplications:Injection moldingConnectors, linkersRelay, bobbins, plugsHousehold appliance parts.. |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical LUMAX GP5306F PBT+ABS+GF30%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF30%, Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4Information provided by LG .. |
|||
Middle Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP2156FL PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant Application: IT/OA, E&E (CRT Socket)CAS No. 68928-70-1, 71342-77-3, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by.. |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP2300R PBT+GF30% Description: Injection Molding, PBT+GF30%, Anti-HydrolysisApplication: E&E (Speed Nut & Body)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP2306FB PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP2306FC PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP2306FI PBT+GF30% Description: Injection Molding, PBT+GF30%, Flame Retardant, High Impact Application: IT/OA, E&E (Connector)CAS No. 68928-70-1, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical.. |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® SG3250 PBT+PET+MF25% Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® SV1120M PBT Description: Injection Molding, PBT, General Purpose, High ViscosityApplication: Films & Sheets, Optical Loose TubeCAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 °C | 464 °F | |
Multibase Multi-Flex® D 5304 Black TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | |
Lavergne VYTEEN PC/ABS 3016 PC-ABS, 16% Glass Reinforced Vyteen PC/ABS 3016 is a black 16% glass fiber reinforced Polycarbonate/ABS alloy designed for injection molding.Features: -Good processability -Balanced stiffness/resilience -High deflection temp.. |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical Lupox® GP2156FT PBT+GF15% Description: Injection Molding, PBT+GF15%, Flame Retardant, High FlowApplication: IT/OA, E&E (Connector)CAS No. 71342-77-3, 65997-17-3, 24968-12-5 and 1309-64-4Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 255 °C | 464 - 491 °F | Injection Molding |
LG Chemical LUPOY ER5001RFA PC/ABS, Halogen Free, Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EPEATApplication: IT&OA (Notebook PC housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 255 °C | 464 - 491 °F | Injection Molding |
LG Chemical LUPOY GN5001EF PC/ABS, Br, Cal-free flame retardant Description: Injection Molding, PC/ABS, Halogen Free Flame RetardantApplication: Industrial / IT productCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 240 - 280 °C | 464 - 536 °F | Injection Molding |
Styrolution Luran® S 777 K ASA Luran S 777 K is an easy flowing injection molding ASA grade with good toughness and heat distorsion resistance. |
|||
Middle Barrel Temperature | 240 - 280 °C | 464 - 536 °F | |
Teknor Apex Beetle® MDF2 Nylon 6, 30% Short Glass Fiber Reinforced, Dry Notes: MDF2 is a heat stabilized 30% glass fiber reinforced nylon 6 that offers good mechanical performance coupled with good surface finish. Features: Heat Stabilized; Good Surface Finish Processin.. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | |
Unitika AXF-1500-05 Dry Characteristics: Lubricant grade of AX1500, excellent in heat and chemical resistancesInformation provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | |
Unitika LM-8503-10 Chemical resistance, and excellent lubricant propertyInformation provided by Unitika Ltd. |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Zone 2 |
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Zone 2 |
Eurostar Staramide PF004EUC PA6, 20% Glass Filled, Injection Molded PF004EUC is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Middle Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Zone 2 |
Eurostar Staramide BG6 PA6, 30% Glass Filled, Injection Molded BG6 is a 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Middle Barrel Temperature | 240 - 270 °C | 464 - 518 °F | |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Middle Barrel Temperature | 240 - 270 °C | 464 - 518 °F | |
Ascend Performance Materials Vydyne® 909 Nylon 66/6, 25% Glass Reinforced, Ignition Resistant, DAM Vydyne® 909 is halogenated, 25% glass-filled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwriters.. |
|||
Middle Barrel Temperature | 240 - 280 °C | 464 - 536 °F | Cylinder Temperature |
Asia International Enterprise (Hong Kong) ST6010 Nylon 66 Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Middle Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Start Point: 245°C |
Kingfa JE2-R2G30 Glass Fiber Reinforced ABS/PBT Alloy Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a.. |