Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 220 °C | 428 °F | Zone 3; Cylinder |
Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Zone 4; Cylinder |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Zone 4; Cylinder |
Premix Thermoplastics PRE-ELEC® PET 1451 PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Zone 3; Cylinder |
Premix Thermoplastics PRE-ELEC® PP 1386 PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Zone 3; Cylinder |
Premix Thermoplastics PRE-ELEC® PS 1324 PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Zone 3; Cylinder |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | |
Gichem GILAC E200 Acrylonitrile Butadiene Styrene
(discontinued **) ABS medium fluidity, excellent resilience. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Middle Barrel Temperature | 220 °C | 428 °F | |
Gichem GILAC D160/MT Acrylonitrile Butadiene Styrene
(discontinued **) ABS with good resilience, good thermal properties. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Middle Barrel Temperature | 220 °C | 428 °F | |
DuPont Bynel® 30E699 Adhesive Resin
(discontinued **) Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa MAC-501 Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Start Point: 235°C |
Kingfa MAC-751 HF PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT 1163D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | |
LG Chemical LUMAX HF-5008 High Flow PBT, Dimensional Stability LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | |
Gromax 1155LL TPE 1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex.. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Start Point: 240°C |
Kingfa MAC-451 UV Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Start Point: 240°C |
Kingfa MAC-451PG Electroplating PC/ABS Alloy Features:Excellent balance propertiesGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank coverComputer and accessor.. |
|||
Middle Barrel Temperature | 220 - 275 °C | 428 - 527 °F | Injection Molding |
LG Chemical LUPOY GN5001RFD PC/ABS, High Impact Description: Injection Molding, PC/ABS, General Purpose, High Impact, Halogen Free Flame retardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | |
Samyang Triloy® 120H PC/ABS alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityGood flowApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | |
Samyang Triloy® 170 PC/PBT alloy Characteristics:Impact resistantChemical resistantDimensional stabilityProcessabilityFlame retardantApplications:Automotive bumperAutomotive outdoor handleAll information provided by Samyang |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Extrusion lamination |
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent .. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Extrusion lamination |
DuPont Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3117 AC is intended for coextrusion and compounding. Due to its high melt flow rate, it is used also in extrusion coating. Elvaloy® 3117 AC is soft, flexible and has good adhesion to va.. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Mid-2. Region Temperature |
Tisan TISESTER® 30% Glass Fiber Reinforced and heat Stabilized Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Mid-2. Region Temperature |
Tisan TISESTER® 30% Glass Fiber Reinforced, Flame Retardant (V0). Heat Stabilized. Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Mid-2. Region Temperature |
Tisan TISESTER® 30% Glass Fiber Reinforced, Impact Resistance and Heat Stabilized ISI Stab. Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Mid-2. Region Temperature |
Tisan TISESTER® Flame Retardant (V0). Heat Stabilized Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Mid-2. Region Temperature |
Tisan TISLAMID® 6 15% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Mid-2. Region Temperature |
Tisan TISLAMID® 6 30% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | |
DuPont Bynel® 30E670 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Extrusion lamination |
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |